Process for demineralizing a sugar-containing solution
    1.
    发明授权
    Process for demineralizing a sugar-containing solution 失效
    含糖溶液脱矿质的方法

    公开(公告)号:US5094694A

    公开(公告)日:1992-03-10

    申请号:US668395

    申请日:1991-03-13

    IPC分类号: C13B20/14 C13K11/00

    CPC分类号: C13B20/14 C13K11/00

    摘要: Improved method for demineralizing a sugar-containing solution using an ion exchange resin in bead form wherein the volume average bead diameter is from 400 to 700 .mu.m and the bead diameter distribution is such that at least 80 volume percent of the beads have diameters which fall within a range of .+-.15 percent of the volume average diameter of the resin used.

    摘要翻译: 使用珠粒形式的离子交换树脂使含糖溶液脱矿质的改进方法,其中体积平均珠粒直径为400-700μm,珠粒直径分布使得至少80体积%的珠具有直径下降 在所用树脂的体积平均直径的±15%的范围内。