POLYMER ELECTROLYTE MEMBRANE AND MEMBRANE/ELECTRODE ASSEMBLY FOR POLYMER ELECTROLYTE FUEL CELL
    1.
    发明申请
    POLYMER ELECTROLYTE MEMBRANE AND MEMBRANE/ELECTRODE ASSEMBLY FOR POLYMER ELECTROLYTE FUEL CELL 有权
    聚合物电解质膜和膜/电极组件聚合物电解质燃料电池

    公开(公告)号:US20080166601A1

    公开(公告)日:2008-07-10

    申请号:US11971450

    申请日:2008-01-09

    IPC分类号: H01M8/10

    摘要: A membrane/electrode assembly for a polymer electrolyte fuel cell capable of exhibiting high power generation performance constantly for a long period of time in a high temperature and low humidity environment, and a polymer electrolyte membrane whereby such a membrane/electrode assembly is obtainable.A polymer electrode membrane 15, comprising a proton conductive polymer which has an electrical conductivity of at least 0.07 S/cm at a temperature of 80° C. at a relative humidity of 40% and which has a water content of less than 15 mass; and a membrane/electrode assembly 10 comprising an anode 13 and a cathode 14 each having a catalyst layer 11, and a polymer electrolyte membrane 15 disposed between the anode 13 and the cathode 14.

    摘要翻译: 一种能够在高温低湿环境下长时间持续显示高发电性能的聚合物电解质型燃料电池用膜/电极接合体,能够得到这样的膜/电极接合体的高分子电解质膜。 聚合物电极膜15,其包含质子传导性聚合物,其在相对湿度为40%且水含量小于15质量%的情况下,在80℃的温度下具有至少0.07S / cm的导电率; 以及包括具有催化剂层11的阳极13和阴极14以及设置在阳极13和阴极14之间的聚合物电解质膜15的膜/电极组件10。

    POLYMER ELECTROLYTE MEMBRANE FOR POLYMER ELECTROLYTE FUEL CELLS, AND MEMBRANE/ELECTRODE ASSEMBLY
    3.
    发明申请
    POLYMER ELECTROLYTE MEMBRANE FOR POLYMER ELECTROLYTE FUEL CELLS, AND MEMBRANE/ELECTRODE ASSEMBLY 审中-公开
    用于聚合物电解质燃料电池的聚合物电解质膜和膜/电极组件

    公开(公告)号:US20080138686A1

    公开(公告)日:2008-06-12

    申请号:US12023242

    申请日:2008-01-31

    IPC分类号: H01M8/10 C08J5/22

    摘要: To provide a polymer electrolyte membrane for polymer electrolyte fuel cells, which is less likely to be broken even when it undergoes repetition of swelling in a wet state and shrinkage in a dry state and a membrane/electrode assembly using it.To provide a polymer electrolyte membrane 15 in which the tensile yield stress obtained from the tensile stress-strain curve in accordance with the tensile test according to JIS K 7161-1994 at a temperature of 80° C. at a strain rate of 1/min and by means of an evaluation method according to JIS K 7161-1994, is at most 5.5 MPa; and a membrane/electrode assembly 10 having the polymer electrolyte membrane 15 disposed between an anode 13 and a cathode 14 each having a catalyst layer 11.

    摘要翻译: 为了提供聚合物电解质燃料电池用高分子电解质膜,即使在湿状态下发生膨胀,干燥状态下收缩也不容易破裂,也可以使用该高分子电解质膜。 提供一种聚合物电解质膜15,其中拉伸应力 - 应变曲线根据JIS K 7161-1994的拉伸试验获得的拉伸屈服应力在80℃的温度下以1 / min的应变速率 根据JIS K 7161-1994的评价方法,最高为5.5MPa; 以及具有设置在各自具有催化剂层11的阳极13和阴极14之间的聚合物电解质膜15的膜/电极组件10。