POLYMER ELECTROLYTE MEMBRANE FOR POLYMER ELECTROLYTE FUEL CELLS, AND MEMBRANE/ELECTRODE ASSEMBLY
    1.
    发明申请
    POLYMER ELECTROLYTE MEMBRANE FOR POLYMER ELECTROLYTE FUEL CELLS, AND MEMBRANE/ELECTRODE ASSEMBLY 审中-公开
    用于聚合物电解质燃料电池的聚合物电解质膜和膜/电极组件

    公开(公告)号:US20080138686A1

    公开(公告)日:2008-06-12

    申请号:US12023242

    申请日:2008-01-31

    IPC分类号: H01M8/10 C08J5/22

    摘要: To provide a polymer electrolyte membrane for polymer electrolyte fuel cells, which is less likely to be broken even when it undergoes repetition of swelling in a wet state and shrinkage in a dry state and a membrane/electrode assembly using it.To provide a polymer electrolyte membrane 15 in which the tensile yield stress obtained from the tensile stress-strain curve in accordance with the tensile test according to JIS K 7161-1994 at a temperature of 80° C. at a strain rate of 1/min and by means of an evaluation method according to JIS K 7161-1994, is at most 5.5 MPa; and a membrane/electrode assembly 10 having the polymer electrolyte membrane 15 disposed between an anode 13 and a cathode 14 each having a catalyst layer 11.

    摘要翻译: 为了提供聚合物电解质燃料电池用高分子电解质膜,即使在湿状态下发生膨胀,干燥状态下收缩也不容易破裂,也可以使用该高分子电解质膜。 提供一种聚合物电解质膜15,其中拉伸应力 - 应变曲线根据JIS K 7161-1994的拉伸试验获得的拉伸屈服应力在80℃的温度下以1 / min的应变速率 根据JIS K 7161-1994的评价方法,最高为5.5MPa; 以及具有设置在各自具有催化剂层11的阳极13和阴极14之间的聚合物电解质膜15的膜/电极组件10。