Method for producing a leather semi-finished product
    1.
    发明申请
    Method for producing a leather semi-finished product 失效
    皮革半成品的制造方法

    公开(公告)号:US20060075573A1

    公开(公告)日:2006-04-13

    申请号:US10531178

    申请日:2003-11-25

    IPC分类号: D06M19/00

    CPC分类号: C14C3/16 C14C3/28

    摘要: A semifinished leather product is produced from an animal hide by pretanning with the use of a chromium-free tanning agent and of a clay mineral which, after stirring for 30 minutes in water at 50° C. at a circumferential rotor speed of from 5 to 25 m/s, has a number average particle diameter of less than 2 μm or a bimodal particle size distribution with a first, finely divided fraction whose number average particle diameter is less than 0.5 μm and a second, coarser fraction whose number average particle diameter is less than 5 μm, determined in each case by the method according to ISO 13320-1, by combined laser light diffraction and light scattering, a proportion of the first, finely divided fraction being from 10 to 90% by weight, and drying of the pretanned animal hide to a water content of from 5 to 45% based on the total weight of the semifinished leather product.

    摘要翻译: 通过使用无铬鞣剂和粘土矿物预处理从动物皮制造半成品皮革制品,其在50℃的水中搅拌30分钟,周向转子速度为5至 25m / s,数均粒径小于2μm,或双峰粒径分布,其数均粒径小于0.5μm的第一微细分数,第二较粗颗粒的数均粒径 通过组合的激光衍射和光散射,通过根据ISO 13320-1的方法在每种情况下确定小于5um,一部分细碎部分的比例为10至90重量%,并干燥 基于半成品​​皮革制品的总重量,预制动物的水分含量为5至45%。

    Formulation for use in chrome or chrome-free tannage
    2.
    发明申请
    Formulation for use in chrome or chrome-free tannage 失效
    用于铬或无铬鞣革的配方

    公开(公告)号:US20060101584A1

    公开(公告)日:2006-05-18

    申请号:US10524047

    申请日:2003-08-14

    IPC分类号: C14C3/00

    CPC分类号: C14C3/16 C14C3/28

    摘要: A formulation for use in chrome-free or chrome tanning is proposed, comprising a clay mineral which, after vigorous stirring for 30 minutes in water at 50° C., has a number average particle diameter of less than 2 μm or a bimodal size distribution with a first, finely divided fraction whose number average particle diameter is less than 0.5 μm and a second, coarser fraction whose number average particle diameter is less than 5 μm, determined in each case by the method according to ISO 13320-1, by combined laser light diffraction and light scattering, the amount of the first, finely divided fraction being from 10 to 90% by weight, and one or more substances from one or more of the following groups: organic polymers, aldehyde tanning agents, sulfone tanning agents, resin tanning agents, phenol tanning agents, fatliquoring agents, vegetable tanning agents, dyes and pigments.

    摘要翻译: 提出了用于无铬或铬鞣制剂的制剂,其包含粘土矿物,其在50℃下在水中剧烈搅拌30分钟后具有小于2μm的数均粒径或双峰尺寸分布 具有数均粒径小于0.5μm的第一细碎部分和数均粒径小于5μm的第二粗纱部分,通过组合的方法按照ISO 13320-1的方法确定 激光衍射和光散射,第一细分的份数为10至90重量%,以及一种或多种下列一种或多种物质:​​有机聚合物,醛鞣剂,砜鞣剂, 树脂鞣剂,苯酚鞣剂,加脂剂,植物鞣剂,染料和颜料。

    Method for hydrophobing leather and furskins
    3.
    发明申请
    Method for hydrophobing leather and furskins 审中-公开
    疏水皮革和毛皮的方法

    公开(公告)号:US20060096036A1

    公开(公告)日:2006-05-11

    申请号:US10544785

    申请日:2004-01-28

    IPC分类号: C14C1/00

    CPC分类号: C14C9/02

    摘要: Water repellency is imparted to leather and fur skins by a process in which leather or fur skin is treated, before, during or after the retanning, with one or more formulations comprising from 1 to 30% by weight, based on the formulation, of a mixture of polysiloxanes comprising from 10 to 90% by weight, based on the mixture, of one or more carboxyl-containing polysiloxanes, from 90 to 10% by weight, based on the mixture, of one or more carboxyl-free polysiloxanes and from 3 to 25% by weight, based on the formulation, of at least one emulsifier.

    摘要翻译: 通过在复鞣之前,期间或之后处理皮革或皮毛皮肤的方法赋予皮革和毛皮皮肤防水性,其中一种或多种制剂包含基于制剂的1至30重量% 基于混合物,包含基于混合物的10至90重量%的一种或多种含羧基聚硅氧烷的混合物,基于该混合物的90至1​​0重量%的一种或多种无羧基聚硅氧烷和3 至25重量%,基于配方,至少一种乳化剂。