1.
公开(公告)号:US07045475B2
公开(公告)日:2006-05-16
申请号:US10834147
申请日:2004-04-28
申请人: Ufuk Senturk , Michael P. Lanci , Raymond Jackson , John W. Lau
发明人: Ufuk Senturk , Michael P. Lanci , Raymond Jackson , John W. Lau
CPC分类号: C03C3/078 , C03C12/02 , Y10T428/2982
摘要: Glass formulations, and a method of converting such glass formulations to glass beads having a refractive index of at least 1.59 and a high level of retroreflectivity, are provided. The methods and formulations provide beads also having high levels of resistance to degradation by environmental exposure.
摘要翻译: 提供了玻璃制剂,以及将这种玻璃制剂转化为具有至少1.59的折射率和高反射性水平的玻璃珠的方法。 所述方法和制剂提供珠粒,其还具有高水平的耐环境暴露降解性。
-
公开(公告)号:US20060084724A1
公开(公告)日:2006-04-20
申请号:US10967540
申请日:2004-10-18
申请人: Ufuk Senturk
发明人: Ufuk Senturk
IPC分类号: C08J9/32
CPC分类号: C03C11/002 , C03C11/00 , Y10T428/2982 , Y10T428/2996
摘要: Glass microspheres containing a substantial percentage of spheres having two or more optically visible gas bubbles per sphere provide a high level of whitening to composite materials containing them. The volume of gas bubbles is between 8 and 35 percent of the volume of the spheres on average, and the spheres exhibit good resistance to breakage upon exposure to high pressures such as may be encountered in polymer extrusion processes. The spheres have a median particle diameter of between 5 and 100 μm, and at least 10% by number of the spheres incorporate at least two gas bubbles.
摘要翻译: 含有相当百分比的具有每个球体两个或更多个光学可见气泡的球体的玻璃微球体对含有它们的复合材料提供高水平的增白。 气泡的体积平均为球体体积的8至35%,并且球体在暴露于高压下(例如在聚合物挤出方法中可能遇到的)表现出良好的抗断裂性。 球体的中值粒径在5-100μm之间,并且至少10个数量的球体包含至少两个气泡。
-
公开(公告)号:US07846994B2
公开(公告)日:2010-12-07
申请号:US12342260
申请日:2008-12-23
申请人: Larry Royer , Michael Meshey , Ufuk Senturk
发明人: Larry Royer , Michael Meshey , Ufuk Senturk
IPC分类号: C08K7/16
CPC分类号: C08K7/18 , Y10T428/2982
摘要: This invention relates to inorganic microspheres having a relatively narrow particle size distribution, which may be prepared by spheridization of zeolite crystals. The microspheres are particularly useful for whitening polymer compositions and in other filler applications.
摘要翻译: 本发明涉及具有相对窄的粒度分布的无机微球,其可以通过沸石晶体的球化来制备。 微球对于增白聚合物组合物和其它填料应用是特别有用的。
-
公开(公告)号:US20100160527A1
公开(公告)日:2010-06-24
申请号:US12342260
申请日:2008-12-23
申请人: Larry Royer , Michael Meshey , Ufuk Senturk
发明人: Larry Royer , Michael Meshey , Ufuk Senturk
CPC分类号: C08K7/18 , Y10T428/2982
摘要: This invention relates to inorganic microspheres having a relatively narrow particle size distribution, which may be prepared by spheridization of zeolite crystals. The microspheres are particularly useful for whitening polymer compositions and in other filler applications.
摘要翻译: 本发明涉及具有相对窄的粒度分布的无机微球,其可以通过沸石晶体的球化来制备。 微球对于增白聚合物组合物和其它填料应用是特别有用的。
-
公开(公告)号:US07449503B2
公开(公告)日:2008-11-11
申请号:US10967540
申请日:2004-10-18
申请人: Ufuk Senturk
发明人: Ufuk Senturk
IPC分类号: C08J9/32
CPC分类号: C03C11/002 , C03C11/00 , Y10T428/2982 , Y10T428/2996
摘要: Glass microspheres containing a substantial percentage of spheres having two or more optically visible gas bubbles per sphere provide a high level of whitening to composite materials containing them. The volume of gas bubbles is between 8 and 35 percent of the volume of the spheres on average, and the spheres exhibit good resistance to breakage upon exposure to high pressures such as may be encountered in polymer extrusion processes. The spheres have a median particle diameter of between 5 and 100 μm, and at least 10% by number of the spheres incorporate at least two gas bubbles.
摘要翻译: 含有相当百分比的具有每个球体两个或更多个光学可见气泡的球体的玻璃微球体对含有它们的复合材料提供高水平的增白。 气泡的体积平均为球体体积的8至35%,并且球体在暴露于高压下(例如在聚合物挤出方法中可能遇到的)表现出良好的抗断裂性。 球体的中值粒径在5-100μm之间,并且至少10个数量的球体包含至少两个气泡。
-
6.
公开(公告)号:US20050245642A1
公开(公告)日:2005-11-03
申请号:US10834147
申请日:2004-04-28
申请人: Ufuk Senturk , Michael Lanci , Raymond Jackson , John Lau
发明人: Ufuk Senturk , Michael Lanci , Raymond Jackson , John Lau
IPC分类号: B32B5/16 , C03C20060101 , C03C3/078 , C03C12/02 , C08K3/40
CPC分类号: C03C3/078 , C03C12/02 , Y10T428/2982
摘要: Glass formulations, and a method of converting such glass formulations to glass beads having a refractive index of at least 1.59 and a high level of retroreflectivity, are provided. The methods and formulations provide beads also having high levels of resistance to degradation by environmental exposure.
摘要翻译: 提供了玻璃制剂,以及将这种玻璃制剂转化为具有至少1.59的折射率和高反射性水平的玻璃珠的方法。 所述方法和制剂提供珠粒,其还具有高水平的耐环境暴露降解性。
-
-
-
-
-