Chromium bearing forehearth color concentrate
    2.
    发明申请
    Chromium bearing forehearth color concentrate 有权
    含铬前炉颜色浓缩液

    公开(公告)号:US20050020429A1

    公开(公告)日:2005-01-27

    申请号:US10602533

    申请日:2003-06-24

    申请人: Kenneth Ackerman

    发明人: Kenneth Ackerman

    CPC分类号: C03C1/105 C03C3/064 C03C12/00

    摘要: A forehearth color concentrate comprising a non-smelted agglomerated interspersion of particles for use in coloring, said concentrate comprising by weight from about 50% to about 95% of a glass component and from about 4% to about 50% of a binder, said glass component comprising by weight from about 15% to about 35% chromium oxide. The present invention further provides a method of using the color concentrate.

    摘要翻译: 一种前炉颜色浓缩物,其包含用于着色的未熔融颗粒聚集的间隙,所述浓缩物包含约50%至约95%的玻璃组分和约4%至约50%的粘合剂,所述玻璃 组分包含约15重量%至约35重量%的氧化铬。 本发明还提供了一种使用浓缩色料的方法。

    GLASS CONVERTIBLE TO TRANSPARENT GLASS CERAMICS CONTAINING AlPO{11
    5.
    发明授权
    GLASS CONVERTIBLE TO TRANSPARENT GLASS CERAMICS CONTAINING AlPO{11 失效
    玻璃可转换为含有AlPO的透明玻璃陶瓷{11

    公开(公告)号:US3642504A

    公开(公告)日:1972-02-15

    申请号:US3642504D

    申请日:1968-07-01

    CPC分类号: C03C10/0027

    摘要: Glass ceramics made from an initial glass composition, in weight percent, of SiO2 : 35-70 Al2O3 : 17-32 P2O5 : 5-17 Li2O : 2-5 MgO : 0-4 ZnO : 0-5 TiO2 : 1.5-6 ZrO2 : 0.5-3 Na2O : traces-0.6 As2O3 : 0.5-1.0, where the P2O5 to TiO2 ratio is up to about 4, and where the sum of ZrO2 and TiO2 is at least about 3 weight percent.

    摘要翻译: 由SiO 2:35-70 Al 2 O 3:17-32 P 2 O 5:5-17 Li 2 O:2-5 MgO:0-4 ZnO:0-5 TiO 2:1.5-6 ZrO 2的初始玻璃组成重量百分比制成的玻璃陶瓷 :0.5-3 Na2O:痕量-0.6 As2O3:0.5-1。

    Flexible electrically switchable glazing structure and methods of forming same
    6.
    发明申请
    Flexible electrically switchable glazing structure and methods of forming same 审中-公开
    柔性电开关玻璃结构及其形成方法

    公开(公告)号:US20050211699A1

    公开(公告)日:2005-09-29

    申请号:US10523494

    申请日:2003-08-04

    摘要: Flexible electrically switchable panels or glazing structures and methods of manufacturing such flexible electrically switchable panels or glazing structures are provided. Particularly, methods and processes are disclosed that enable fast and efficient cutting and shaping of flexible glazing structures into any desired shape and size. In certain embodiments, methods and processes are disclosed whereby barrier lines are formed to define regular or irregular cutting lines and seals. In further embodiments, methods and processes are disclosed whereby notches are defined to expose upper and lower substrate conductive surfaces. In still further embodiments, methods and processes are disclosed whereby glazing structures of irregular shapes and sizes are formed.

    摘要翻译: 提供了柔性电可切换面板或玻璃窗结构以及制造这种柔性电气可切换面板或玻璃窗结构的方法。 特别地,公开了能够将柔性玻璃结构快速有效地切割和成形为任何所需形状和尺寸的方法和方法。 在某些实施例中,公开了方法和方法,其中形成阻挡线以限定规则的或不规则的切割线和密封。 在另外的实施例中,公开了方法和方法,其中限定凹口以暴露上基板导电表面和下基板导电表面。 在另外的实施例中,公开了形成不规则形状和尺寸的玻璃结构的方法和方法。

    Saline soluble inorganic fibers
    7.
    发明申请
    Saline soluble inorganic fibers 失效
    盐水可溶性无机纤维

    公开(公告)号:US20050014624A1

    公开(公告)日:2005-01-20

    申请号:US10833413

    申请日:2004-04-28

    CPC分类号: C03C13/00 C03C2213/02

    摘要: Disclosed is use of a vitreous inorganic fiber in the knowledge that it has a composition meeting the criterion that the calculated sum of the free energies of hydration of the compounds that would or could be present at equilibrium (on the basis of knowledge, informed belief or reasonable assumption) is more negative than −10 kcal/100 grams of composition. Such compositions are saline soluble.

    摘要翻译: 公开了使用玻璃质无机纤维,其知道它具有满足以下标准的组成的组合:所计算的化合物的水合自由能的总和可以或可以以平衡存在(基于知识,知情的信念或 合理的假设)比-10 kcal / 100克的组合更负。 这样的组合物是盐溶性的。

    Amorphous and nanocrystalline glass-coated articles
    8.
    发明申请
    Amorphous and nanocrystalline glass-coated articles 审中-公开
    无定形和纳米晶玻璃涂层制品

    公开(公告)号:US20050000599A1

    公开(公告)日:2005-01-06

    申请号:US10881760

    申请日:2004-06-30

    摘要: A drawn glass-coated metallic member has a thermal contraction coefficient differential such that the thermal contraction coefficient of the glass is less than that of the metallic member. The thermal contraction coefficient differential is maintained within a predetermined range during drawing. The glass is placed under residual compression, interfacial bonding between said glass and said wire is substantially uniform, and surface cracking and bond breaks between metal and glass are substantially prevented. A dynamic balance is maintained between the surface tension of the molten alloy and the resistance to high temperature deformation by the glass vessel in which it is contained, enabling the production of glass-coated amorphous or nanocrystalline alloy members having predefined cross-sectional shapes.

    摘要翻译: 拉制的玻璃涂覆的金属构件具有热收缩系数差,使得玻璃的热收缩系数小于金属构件的热收缩系数。 在拉伸期间,热收缩系数差保持在预定范围内。 将玻璃置于残余压缩之下,所述玻璃与所述丝之间的界面结合基本上是均匀的,并且基本上防止了金属和玻璃之间的表面裂纹和结合断裂。 熔融合金的表面张力与容纳玻璃容器的耐高温变形性之间保持动态平衡,能够生产具有预定横截面形状的玻璃涂覆的非晶或纳米晶合金构件。

    Liquid, radiation-curable coating composition for the coating of glass
surfaces
    9.
    发明授权
    Liquid, radiation-curable coating composition for the coating of glass surfaces 失效
    液体,玻璃表面涂层的可辐射固化涂料组合物

    公开(公告)号:US5229433A

    公开(公告)日:1993-07-20

    申请号:US775975

    申请日:1991-11-28

    摘要: The present invention relates to a liquid, radiation-curable coating composition for the coating of glass surfaces which comprisesA) 56 to 89% by weight of at least one diethylenically unsaturated polyurethane optionally containing urea groups,B) 3 to 30% by weight of at least one ethylenically unsaturated monomer,C) 0.5 to 8% by weight of at least one photoinitiator andD) 0.05 to 6% by weight of an alkoxysilane,the sum total of the components A to D being 100% by weight in each case.The coating composition uses1.) one or more ethylenically unsaturated monomers containing carboxyl groups, optionally together with other ethylenically unsaturated monomers as the component B and2.) an alkoxysilane containing epoxide groups as the component D.These coating compositions are employed for the coating of glass surfaces, in particular of optical glass fibers, and are distinguished by good adhesion even under humid conditions.

    摘要翻译: PCT No.PCT / EP90 / 00520 Sec。 371日期1991年11月28日 102(e)日期1991年11月28日PCT 1990年4月3日PCT PCT。 第WO90 / 13523号公报 1990年11月15日。本发明涉及用于涂覆玻璃表面的液体可辐射固化涂料组合物,其包含A)56至89重量%的至少一种任选含有脲基团的烯属不饱和聚氨酯,B) 3至30重量%的至少一种烯属不饱和单体,C)0.5至8重量%的至少一种光引发剂和D)0.05至6重量%的烷氧基硅烷,组分A至D的总和为 在每种情况下为100重量%。 涂料组合物使用1.)含有羧基的一种或多种烯属不饱和单体,任选地与其它烯属不饱和单体一起作为组分B和2.)含有环氧基作为组分D的烷氧基硅烷。这些涂料组合物用于涂料 的玻璃表面,特别是光学玻璃纤维,并且即使在潮湿条件下也具有良好的粘附性。