Abstract:
A copolymer suitable for use in forming a solid polymer electrolyte film comprising a first monomer represented by Formula (1): wherein n is 2 to 1,000; m is 2 to 1,000; x and y are individually 1 to 100; p is 0 to 10; and q is 1 to 10, R1 is an alkyl group having 1 to 10 carbon atoms, and A is an alkyl acryloyl group an acryloyl group, alkyl acryloyl group, methacryloyl group, alkyl methacryloyl group, a vinyl group, an allyl group, a styryl group, or a combination of two or more thereof; and a second monomer chosen from a hydroxyl-substituted alkyl acrylate, a hydroxyl-substituted alkyl methacrylate, or a combination of two or more thereof. The copolymer may be used to form a solid polymer electrolyte composition comprising (i) the copolymer, (ii) a plasticizer, and (iii) a salt. The solid polymer electrolyte may be used to form a solid polymer electrolyte film, which may be suitable for use in electrochemical devices.
Abstract:
A copolymer suitable for use in forming a solid polymer electrolyte film comprising a first monomer represented by Formula (1): wherein n is 2 to 1,000; m is 2 to 1,000; x and y are individually 1 to 100; p is 0 to 10; and q is 1 to 10, R1 is an alkyl group having 1 to 10 carbon atoms, and A is an alkyl acryloyl group an acryloyl group, alkyl acryloyl group, methacryloyl group, alkyl methacryloyl group, a vinyl group, an allyl group, a styryl group, or a combination of two or more thereof; and a second monomer chosen from a hydroxyl-substituted alkyl acrylate, a hydroxyl-substituted alkyl methacrylate, or a combination of two or more thereof. The copolymer may be used to form a solid polymer electrolyte composition comprising (i) the copolymer, (ii) a plasticizer, and (iii) a salt. The solid polymer electrolyte may be used to form a solid polymer electrolyte film, which may be suitable for use in electrochemical devices.
Abstract:
Disclosed herein is a process for making 1,2,4-trivinylcyclohexane that is enriched in a particular geometric isomer. The process involves the thermal isomerization of 1,5,9-cyclododecatriene at temperature between 400° C. and 600° C. followed by an equilibration of the resultant intermediate in either the gas phase or liquid phase at temperature between 180° C. and 375° C. and at pressures ranging from 0.101 kPa to 1,013 kPa. Also disclosed are 1,2,4-trivinylcyclohexane compositions that are enriched in a particular geometric isomer.
Abstract:
Disclosed herein is a process for making 1,2,4-trivinylcyclohexane that is enriched in a particular geometric isomer. The process involves the thermal isomerization of 1,5,9-cyclododecatriene at temperature between 400° C. and 600° C. followed by an equilibration of the resultant intermediate in either the gas phase or liquid phase at temperature between 180° C. and 375° C. and at pressures ranging from 0.101 kPa to 1.013 kPa. Also disclosed are 1,2,4-trivinylcyclohexane compositions that are enriched in a particular geometric isomer.