Nucleating agent composition for enhancing rigidity and toughness of polypropylene
    1.
    发明授权
    Nucleating agent composition for enhancing rigidity and toughness of polypropylene 有权
    用于提高聚丙烯刚性和韧性的成核剂组合物

    公开(公告)号:US09085683B2

    公开(公告)日:2015-07-21

    申请号:US13642350

    申请日:2011-04-19

    申请人: Wen-lin Zhao

    发明人: Wen-lin Zhao

    摘要: A nucleating agent composition for increasing rigidity and toughness of polypropylene is provided. The nucleating agent composition comprises a carboxylate nucleating agent and a phosphate nucleating agent. The carboxylate nucleating agent is selected from the group consisting of sodium benzoate and hydroxyl aluminum para-tertiary butyl benzoate, and the phosphate nucleating agent is selected from any one of sodium 2,2′-methylene-di(4,6-di-t-butyl phenyl) phosphate and aluminum bis[2,2′-methylene-di(4,6-di-t-butylphenyl)] phosphate. The nucleating agent composition according to the present invention not only can significantly improve the bending modulus and thermal deformation temperature of polypropylene, but also can improve the impact strength of polypropylene.

    摘要翻译: 提供了用于提高聚丙烯的刚性和韧性的成核剂组合物。 成核剂组合物包含羧酸盐成核剂和磷酸盐成核剂。 羧酸盐成核剂选自苯甲酸钠和对羟基苯甲酸羟基铝,磷酸盐成核剂选自2,2'-亚甲基二(4,6-di-t) 丁基苯基)磷酸酯和双[2,2'-亚甲基 - 二(4,6-二叔丁基苯基)]磷酸铝。 根据本发明的成核剂组合物不仅可以显着提高聚丙烯的弯曲模量和热变形温度,而且可以提高聚丙烯的冲击强度。

    NUCLEATING AGENT COMPOSITION FOR ENHANCING RIGIDITY AND TOUGHNESS OF POLYPROPYLENE
    2.
    发明申请
    NUCLEATING AGENT COMPOSITION FOR ENHANCING RIGIDITY AND TOUGHNESS OF POLYPROPYLENE 有权
    用于增强聚丙烯的刚性和韧性的核化剂组合物

    公开(公告)号:US20130037743A1

    公开(公告)日:2013-02-14

    申请号:US13642350

    申请日:2011-04-19

    申请人: Wen-lin Zhao

    发明人: Wen-lin Zhao

    IPC分类号: C09K3/00

    摘要: A nucleating agent composition for increasing rigidity and toughness of polypropylene is provided. The nucleating agent composition comprises a carboxylate nucleating agent and a phosphate nucleating agent. The carboxylate nucleating agent is selected from the group consisting of sodium benzoate and hydroxyl aluminum para-tertiary butyl benzoate, and the phosphate nucleating agent is selected from any one of sodium 2,2′-methylene-di(4,6-di-t-butyl phenyl) phosphate and aluminum bis[2,2′-methylene-di(4,6-di-t-butylphenyl)] phosphate. The nucleating agent composition according to the present invention not only can significantly improve the bending modulus and thermal deformation temperature of polypropylene, but also can improve the impact strength of polypropylene.

    摘要翻译: 提供了用于提高聚丙烯的刚性和韧性的成核剂组合物。 成核剂组合物包含羧酸盐成核剂和磷酸盐成核剂。 羧酸盐成核剂选自苯甲酸钠和对羟基苯甲酸羟基铝,磷酸盐成核剂选自2,2'-亚甲基二(4,6-di-t) 丁基苯基)磷酸酯和双[2,2'-亚甲基 - 二(4,6-二叔丁基苯基)]磷酸铝。 根据本发明的成核剂组合物不仅可以显着提高聚丙烯的弯曲模量和热变形温度,而且可以提高聚丙烯的冲击强度。