摘要:
A toner comprising toner particles having at least one type of surface additive, the toner particles having an FPIA average circularity of at least 0.95, whereby at least 80% wt of the total amount of surface additives stays onto the surface of the toner particles when an ultrasonic treatment of 4500 to 4700 J/gram of toner is applied; a substrate printed or marked with the above-described toner; and a method for manufacturing a toner, said method including the steps of: mixing a binder resin, a colorant and optionally other additives, thereby forming a mixture, melting, kneading and milling said mixture, thereby obtaining a melted kneaded product, pulverizing said melted kneaded product, adding at least one surface additive before or while bringing the FPIA average circularity of said toner particles to 0.95 by modifying the shape or surface of said particles, wherein the total amount of surface additive does not exceed 2% wt of toner particles, whereby at least 80% wt of the total amount of surface additive stays on the surface of the toner particles when an ultrasonic treatment of 4500 to 4700 J/gram of toner is applied.
摘要:
A toner comprising toner particles having at least one type of surface additive, the toner particles having an FPIA average circularity of at least 0.95, whereby at least 80% wt of the total amount of surface additives stays onto the surface of the toner particles when an ultrasonic treatment of 4500 to 4700 J/gram of toner is applied; a substrate printed or marked with the above-described toner; and a method for manufacturing a toner, said method including the steps of: mixing a binder resin, a colorant and optionally other additives, thereby forming a mixture, melting, kneading and milling said mixture, thereby obtaining a melted kneaded product, pulverizing said melted kneaded product, adding at least one surface additive before or while bringing the FPIA average circularity of said toner particles to 0.95 by modifying the shape or surface of said particles, wherein the total amount of surface additive does not exceed 2% wt of toner particles, whereby at least 80% wt of the total amount of surface additive stays on the surface of the toner particles when an ultrasonic treatment of 4500 to 4700 J/gram of toner is applied.
摘要:
The present invention provides dry toner particles comprising at least a radiation curable resin, and a colouring agent, wherein the circularity of the toner particles is between 0.95 and 0.99 and a charge control agent in a concentration between 0.025% and 1.0% by weight is present preferably as an external additive.The toners of this invention are useful for printing any substrate and for use in any form of printing or marking device.
摘要:
A radiation curable toner is described comprising at least a radiation curable binder (e.g. a UV curable polymer), a photoinitiator, and a wax; wherein the wax is present in a concentration ranging from 0.3 to 3% by weight. The ratio of scratch resistance after curing to scratch resistance before curing is preferably at least 2.The toner may be used in a developer, e.g. a two-component developer, for printing or copying.
摘要:
The invention relates to dry toner particles comprising at least a radiation curable resin and a colouring agent, the radiation curable resin comprises a blend of a) an (meth)acrylated epoxy/polyester resin b) (meth)acrylated polyurethane resin. Preferably, when fused and cured toner images obtainable from said dry toner particles are obtained on a substrate used for developing same, these images have an equivalent rub number (ERN)>6, wherein ERN=MEK rub resistance/(radiation dose*meq/gr), wherein meq/gr designates the milli-equivalent amount of double bounds per gram of said radiation curable resin and a viscosity behaviour such that the viscosity at 140° C. is lower than the viscosity at 120° C.
摘要:
The present invention relates to a dry toner composition suited for development of electrostatic charge images, magnetic patterns or DEP (Direct Electrostatic Printing). More specifically the present invention relates to a specific toner composition allowing fusing of the toner image to the final substrate at low temperature.
摘要:
Dry toner particles are provided wherein the toner resin includes a mixture of two polymer A and B, A and B being chosen such that an extruded slab with thickness 250 &mgr;m of a 50:50 mixture of both has a transmission density (DM) being between 0.10 and 1.00 higher than the sum of half the transmission density of a 250 &mgr;m extruded slab of polymer A alone (DA) and half the transmission density of a 250 &mgr;m extruded slab of polymer B alone (DB). The polymers A and B are mixed in a weight ratio between 5:1 to 1:5 and make up at least 25% by weight of the total toner resin. The polymer A is a polyester and the polymer B is a polyester or a specified styrene-acrylic copolymer.
摘要:
A dry powder toner of which the particles are electrostatically or magnetically attractable and suited for development of electrostatic charge images or magnetic patterns and wherein the composition of said powder particles includes a resin binder comprising at least one resin A and at least one resin B, characterized in that:(1) said resin(s) A and said resin(s) B each have a glass transition temperature (Tg) larger than 45.degree. C.,(2) the Tg of said resin(s) A is at least 2.5.degree. C. lower than the Tg of said resin(s) B,(3) the melt viscosity (mvA) of said resin(s) A is at least 500 poise and the melt viscosity (mvB) of said resin(s) B is within the scope of the following equation:(mvB)=F.times.(mvA), wherein F is an integer from 2 to 20, and with a maximum value of (mvB) not exceeding 15000 poise, and(4) the weight ratio of resin(s) A and resin(s) B in said powder particles is such that the deformability of the powder material as defined by test H herein is smaller than 15%.
摘要:
An amorphous complex macromolecular compound is provided hat comprises in its macromolecular structure,(i) an amorphous polycondensation backbone, the corresponding backbone polymer having a Tg of at least 45.degree. C. and(ii) at least one polymer chain attached to the backbone, either terminally and/or in a side-chain, this polymer chain being derived from a polymer which on itself has an average molecular weight by number (M.sub.avg) so that 400.ltoreq.M.sub.avg .ltoreq.4000, a melting point between 50.degree. C. and 150.degree. C. and a melting range of at most 15.degree. C.There are also provided methods for the production of the amorphous complex macromolecular compound.Further are provided toner particles and toner receiving substrates comprising the amorphous complex macromolecular compound mentioned above.
摘要:
There are provided dry toner particles wherein the toner resin comprises more than 10% by weight of one or more polysiloxane modified resins. In this resin the polysiloxane moieties are attached to the other polymeric moieties (POL) of said copolymer over an ether group or an ester group. In a preferred embodiment the toner resin of the dry toner particles consists of one or more polysiloxane modified resins.