摘要:
An aluminum alloy, an aluminum alloy wire, an aluminum alloy stranded wire, a covered electric wire, and a wire harness that are of high toughness and high electrical conductivity, and a method of manufacturing an aluminum alloy wire are provided. The aluminum alloy wire contains not less than 0.005% and not more than 2.2% by mass of Fe, and a remainder including Al and an impurity. It may further contain not less than 0.005% and not more than 1.0% by mass in total of at least one additive element selected from Mg, Si, Cu, Zn, Ni, Mn, Ag, Cr, and Zr. The Al alloy wire has an electrical conductivity of not less than 58% IACS and an elongation of not less than 10%. The Al alloy wire is manufactured through the successive steps of casting, rolling, wiredrawing, and softening treatment. The softening treatment can be performed to provide an excellent toughness such as elongation and impact resistance and thereby reduce fracture of the electric wire in the vicinity of a terminal portion when the wire harness is installed.
摘要:
An aluminum alloy, an aluminum alloy wire, an aluminum alloy stranded wire, a covered electric wire, and a wire harness that are of high toughness and high electrical conductivity, and a method of manufacturing an aluminum alloy wire are provided. The aluminum alloy wire contains not less than 0.005% and not more than 2.2% by mass of Fe, and a remainder including Al and an impurity. It may further contain not less than 0.005% and not more than 1.0% by mass in total of at least one additive element selected from Mg, Si, Cu, Zn, Ni, Mn, Ag, Cr, and Zr. The Al alloy wire has an electrical conductivity of not less than 58% IACS and an elongation of not less than 10%. The Al alloy wire is manufactured through the successive steps of casting, rolling, wiredrawing, and softening treatment. The softening treatment can be performed to provide an excellent toughness such as elongation and impact resistance and thereby reduce fracture of the electric wire in the vicinity of a terminal portion when the wire harness is installed.
摘要:
Provided are an aluminum alloy having high toughness and high electric conductivity, an aluminum alloy wire, an aluminum alloy stranded wire, a covered electric wire, a wire harness, and a process for production of an aluminum alloy wire. The aluminum alloy wire contains by mass 0.2 to 1.0% of Mg, 0.1 to 1.0% of Si, and 0.1 to 0.5% of Cu with the balance being Al and impurities and satisfies the relationship: 0.8≦Mg/Si mass ratio≦2.7. The Al alloy wire exhibits an electric conductivity of 58% IACS or above and an elongation of 10% or above. The Al alloy wire is produced via successive steps of casting, rolling, wire drawing, and softening treatment. Since the Al alloy wire has been subjected to softening treatment, the wire is excellent in toughnesses such as elongation and impact resistance, so that when used in a wire harness, the wire is inhibited from being broken in the neighborhood of a terminal in mounting the wire harness.
摘要:
An aluminum alloy wire, an aluminum alloy stranded wire, a covered electric wire, and a wire harness that are of high toughness and high electrical conductivity, and a method of manufacturing an aluminum alloy wire. The aluminum alloy wire contains not less than 0.2% and not more than 1.0% by mass of Mg, not less than 0.1% and not more than 1.0% by mass of Si, not less than 0.1% and not more than 0.5% by mass of Cu, and a remainder including Al and an impurity, and satisfies 0.8 Mg/Si≦2.7 by mass ratio. The Al alloy wire is manufactured through the successive steps of casting, rolling, wiredrawing, and softening treatment.
摘要翻译:具有高韧性和高导电性的铝合金线,铝合金绞线,覆盖电线和线束,以及铝合金线的制造方法。 铝合金线含有不小于0.2%且不大于1.0质量%的Mg,不小于0.1%且不大于1.0质量%的Si,不小于0.1%且不大于0.5质量% 的Cu,余量包括Al和杂质,并且按质量比满足0.8Mg / Si 2 2.7。 Al合金线通过铸造,轧制,拉丝和软化处理的连续步骤制造。
摘要:
A punch guiding apparatus includes: a cylindrical punch guide to be vertically movably supported into a punch holder; a stripper plate is detachably mounted to a forward end portion of the cylindrical punch guide; and a ring-shaped fixture. In the construction, the fixture has a ring shape that both ends are brought into contact with or close to each other. Furthermore, the fixture has a non-circular shape in which it has a plurality of elastically deformed portions which are urged and come in contact with an inner peripheral surface of the punch guide so as to be enlarged.
摘要:
There is provided a method comprising a process of lightly fitting a distal end portion of a projecting portion 25 of a blank holder 23 into a fitting groove 19 formed in a punch guide 5 so as to be momentarily held therein; and a process of fitting the projecting portion 25 of the blank holder 23 into the fitting groove 19 while punching a punch guide hole 23G in the blank holder 23 when a punching portion 7 of a punch body 9 of a punch assembly 1 is lowered for pressing the blank holder 23 against a die D so that the punch guide 5 descends. In the punch assembly 1 constructed in a manner that the punch body 9 is vertically movably housed in a punch guide 5, and the blank holder 23 is removably fitted into the fitting groove formed in the punch guide 5, the punch guide 5 and the blank holder 23 are formed with an inclined plane 5S and an inclined plane 23S at part of an outer peripheral face on the lower end portion of the punch guide 5 or part of an upper face of a flange of the blank holder 23, respectively.