公开(公告)号:US20190352790A1
公开(公告)日:2019-11-21
申请号:US16474208
申请日:2017-12-20
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Sarang V. Deodhar , James J. Kobe , Meredith A. Opatz , Vasav Sahni , Daniel C. Munson
Abstract: A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed on the primed surface of the backing layer, wherein the pressure sensitive adhesive layer has a thickness of at least 7.6 micrometers (and preferably up to 25 micrometers); wherein, when disposed on an aluminum substrate, the tape displays a peel adhesion of less than 20 oz/in (219 N/m) according to a Peel Adhesion Strength Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to a Chromic Acid Anodization—Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.
-
公开(公告)号:US20210324243A1
公开(公告)日:2021-10-21
申请号:US17252599
申请日:2019-06-27
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Christopher W. Cox , Sarang V. Deodhar , Albert I. Everaerts , Becky A. Jetto , James J. Kobe , Meredith A. Opatz , Carla S. Thomas
Abstract: A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 25 micrometers; and an acrylic-based pressure sensitive adhesive layer disposed on one major surface of the backing layer, wherein the acrylic-based pressure sensitive adhesive comprises the reaction of one or more (C8-C20)alkyl acrylates with one or more reinforcing monomers having a homopolymer Tg of at least 50° C., wherein the acrylic-based pressure sensitive adhesive has a tan δ of at least 0.5 measured at 80° C. and an oscillating frequency of 1 radian/second, and wherein the acrylic-based pressure sensitive adhesive layer has a thickness of at least 5 micrometers; wherein, when disposed on an aluminum substrate, the tape displays clean removal from the aluminum substrate according to the Clean Removal Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to the Chromic Acid Anodization-Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.
-