公开(公告)号:US10807776B2
公开(公告)日:2020-10-20
申请号:US15909385
申请日:2018-03-01
Applicant: AGC Inc.
Inventor: Daisuke Taguchi , Wataru Kasai , Yoshiaki Higuchi
IPC: B65D59/02 , C08J5/18 , B65D39/00 , C09D123/08 , C08F214/26 , C08F210/02 , C08L23/08 , C08L27/18 , G01N25/48
Abstract: To provide a resin film which comprises an ethylene/tetrafluoroethylene copolymer and which is to be used as, for example, a rubber plug lamination film to prevent breakage at the time of producing a laminated rubber plug. The resin film comprises an ethylene/tetrafluoroethylene copolymer and is characterized in that the product of the value of the endothermic peak height ΔH (mW/mg) obtained by its DSC-analysis and the haze (%) measured at a thickness of 100 μm, is from 0.1 to 0.2 (mW/mg·%).
-
公开(公告)号:US10882936B2
公开(公告)日:2021-01-05
申请号:US15959634
申请日:2018-04-23
Applicant: AGC Inc.
Inventor: Shigeru Aida , Daisuke Taguchi
IPC: C08F214/26 , C08L27/18
Abstract: To provide a copolymer capable of producing a molded article excellent in strength at a high temperature. A copolymer comprising ethylene units, tetrafluoroethylene units and other monomer units, wherein to the sum of ethylene units and tetrafluoroethylene units, the ethylene units are from 49 to 40 mol % and the tetrafluoroethylene units are from 51 to 60 mol %; to all units in the copolymer, other monomer units are from 2.6 to 6.0 mol %; the melting point is at least 230° C.; and the melt flow rate is from 1 to 15 g/10 min.
-