公开(公告)号:US20190085107A1
公开(公告)日:2019-03-21
申请号:US16191768
申请日:2018-11-15
Applicant: AGC Inc.
Inventor: Wataru KASAI , Kengo Kawahara
IPC: C08F214/26 , C08F210/02
Abstract: To provide an ETFE film which is unlikely to wrinkle when stretched and retracted, and a method for producing the same. It is an ethylene-tetrafluoroethylene copolymer film characterized in that the crystallinity obtainable by the formula (1) from the peak area S20 in the vicinity of 2θ=20°, the peak area S19 in the vicinity of 2θ=19° and the peak area S17 in the vicinity of 2θ=17° in the diffraction intensity curve obtainable by the X-ray diffraction method, is from 55 to 70%, and the proportion of the quasi-crystal layer obtainable by the formula (2) is from 10 to 20%: Crystallinity (%)=(S19+S20)/(S17+S19+S20)×100 (1) Proportion of quasi-crystal layer (%)=S20/(S17+S19+S20)×100 (2)
-
公开(公告)号:US10940629B2
公开(公告)日:2021-03-09
申请号:US16191768
申请日:2018-11-15
Applicant: AGC Inc.
Inventor: Wataru Kasai , Kengo Kawahara
IPC: B29C48/885 , C08J5/18 , B29C48/08 , B29C48/305 , B29C48/88 , C08F210/02 , C08F214/26 , B29K627/18 , B29K23/00 , B29K27/18 , B29L7/00 , C08L27/18 , C08L23/08 , B29C48/00 , B29K627/12
Abstract: To provide an ETFE film which is unlikely to wrinkle when stretched and retracted, and a method for producing the same. It is an ethylene-tetrafluoroethylene copolymer film characterized in that the crystallinity obtained by the formula (1) from the peak area S20 in the vicinity of 2θ=20°, the peak area S19 in the vicinity of 2θ=19° and the peak area S17 in the vicinity of 2θ=17° in the diffraction intensity curve obtained by the X-ray diffraction method, is from 55 to 70%, and the proportion of the quasi-crystal layer obtained by the formula (2) is from 10 to 20%: crystallinity (%)=(S19+S2)/(S17+S19+S20)×100 (1) proportion of quasi-crystal layer (%)=S20/(S17+S19++S20)×100 (2).
-