公开(公告)号:US20220298598A1
公开(公告)日:2022-09-22
申请号:US17835347
申请日:2022-06-08
Applicant: ArcelorMittal
Inventor: Rashmi Ranjan MOHANTY , Hyun Jo JUN , Dongwei FAN , Pavan K. C. VENKATASURYA
IPC: C21D9/46 , C22C38/06 , C22C38/14 , C22C38/02 , C22C38/04 , C22C38/12 , C21D9/48 , C21D1/19 , C21D8/04 , C21D1/18 , C21D6/00
Abstract: A steel sheet made of a steel having a chemical composition containing in weight %: 0.13%≤C≤0.22%, 1.2%≤Si≤1.8%, 1.8%≤Mn≤2.2%, 0.10%≤Mo≤0.20%, Nb≤0.05%, Ti≤0.05%, Al≤0.5%, a remainder being Fe and unavoidable impurities. The steel sheet has a yield strength of at least 850 MPa, a tensile strength of at least 1180 MPa, a total elongation of at least 13% and a hole expansion ratio HER of at least 30%.
-
2.
公开(公告)号:US20200224287A1
公开(公告)日:2020-07-16
申请号:US16827696
申请日:2020-03-23
Applicant: ArcelorMittal
Inventor: Dongwei FAN , Hyun Jo JUN , Rashmi MOHANTY , Pavan K. C. VENKATASURYA
IPC: C21D9/46 , C22C38/02 , C22C38/04 , C21D8/02 , C21D1/18 , C21D6/00 , C22C38/06 , C22C38/12 , C22C38/14 , C23C2/06 , C23C2/28 , C23C2/40
Abstract: A method is for producing a high strength coated steel sheet having an improved ductility and an improved formability, and a chemical composition containing: 0.13%≤C≤0.22%, 1.9%≤Si≤2.3%, 2.4%≤Mn≤3%, Al≤0.5%, Ti≤0.05%, Nb≤0.05%, the remainder being Fe and unavoidable impurities. The sheet is annealed at temperature TA higher than Ac3 but less than 1000° C. for a time of more than 30 s, quenched by cooling to a quenching temperature QT between 200° C. and 280° C. in order to obtain a structure consisting of austenite and at least 50% of martensite, the austenite content being such that the final structure can contain between 3% and 15% of residual austenite and between 85% and 97% of the sum of martensite and bainite, without ferrite, heated up to a partitioning temperature PT between 430° C. and 490° C. and maintained at this temperature for a time Pt between 10 s and 100 s, hot dip coated and cooled to the room temperature.
-