Abstract:
A PROCESS IS PROVIDED FOR THE PRODUCTION OF POLYURETHANE ELASTOMERS BY REACTING HIGHER MOLECULAR WEIGHT HYDROXY COMPOUNDS WHICH HAVE A MOLECULAR WEIGHT OF 800 TO 2500, DIISOCYANATES AND LOW MOLECULAR WEIGHT COMPOUNDS WHICH HAVE A MOLECULAR WEIGHT OF UP TO 400 AND WHICH CONTAIN AT LEAST TWO HYDROGEN ATOMS REACTIVE WITH ISOCYANATES, CHARACTERIZED IN THAT THE HIGHER MOLECULAR WEIGHT HYDROXY COMPOUNDS ARE CONDENSATION PRODUCTS OF 1,6-HEXANE DIOL, ADIPIC ACID AND DIARYL CARBONATE.
Abstract:
TEXTILE FLOOR COVER COATED WITH AN UNFOAMED POLYURETHANE ELASTOMER BASED ON A POLYHYDROXYL COMPOUND SELECTED FROM THE GROUP CONSISTING OF POLYESTES OF ETHYLENE GLYCOL, PROPYLENE GLYCOL, BUTYLENE GLYCOL AND MIXTURES THEREOF, SAID GLYCOLS HAVING TWO OR MORE TERMINAL HYDROXY GROUPS AND AN AVERAGE MOLECULAR WEIGH OF 300-5000 AND A POLYISOCYANATE WITH AN OH/NCO RATIO OF FROM 1:0.3 TO 1:1.3.