COMPOSITIONS AND THEIR USE
    2.
    发明申请
    COMPOSITIONS AND THEIR USE 有权
    组合物及其使用

    公开(公告)号:US20130309424A1

    公开(公告)日:2013-11-21

    申请号:US13982227

    申请日:2011-01-29

    IPC分类号: B41M5/52 B32B37/12

    摘要: A composition includes a mixture including a first polymer and a second polymer. The first polymer includes methyl acrylate or ethyl acrylate residues in an amount of about 15% to about 25% by weight of the first polymer, maleic anhydride residues in an amount of about 2% to about 3.5% by weight of the first polymer, and ethylene residues. The second polymer includes butyl acrylate residues in an amount of about 5% to about 10% by weight of the second polymer, maleic anhydride residues in an amount of about 3% to about 4% by weight of the second polymer, and ethylene residues. An amount of the first polymer in the mixture is about 60% to about 90% by weight. The mixture may further include a pigment-LDPE composition wherein the amount of the first polymer in the mixture is about 50% to about 70% by weight.

    摘要翻译: 组合物包括包含第一聚合物和第二聚合物的混合物。 第一聚合物包括丙烯酸甲酯或丙烯酸乙酯残基的量为第一聚合物的约15重量%至约25重量%,马来酸酐残基的量为第一聚合物的约2重量%至约3.5重量%,以及 乙烯残基。 第二聚合物包括按第二聚合物的重量计约5%至约10%的量的丙烯酸丁酯残基,第二聚合物重量的约3%至约4%的马来酸酐残基和乙烯残基。 混合物中第一聚合物的量为约60重量%至约90重量%。 该混合物可进一步包括颜料-LDPE组合物,其中混合物中第一聚合物的量为约50%至约70%重量。

    Compositions and their use
    5.
    发明授权
    Compositions and their use 有权
    组合及其用途

    公开(公告)号:US08993078B2

    公开(公告)日:2015-03-31

    申请号:US13982227

    申请日:2011-01-29

    摘要: A composition includes a mixture including a first polymer and a second polymer. The first polymer includes methyl acrylate or ethyl acrylate residues in an amount of about 15% to about 25% by weight of the first polymer, maleic anhydride residues in an amount of about 2% to about 3.5% by weight of the first polymer, and ethylene residues. The second polymer includes butyl acrylate residues in an amount of about 5% to about 10% by weight of the second polymer, maleic anhydride residues in an amount of about 3% to about 4% by weight of the second polymer, and ethylene residues. An amount of the first polymer in the mixture is about 60% to about 90% by weight. The mixture may further include a pigment-LDPE composition wherein the amount of the first polymer in the mixture is about 50% to about 70% by weight.

    摘要翻译: 组合物包括包含第一聚合物和第二聚合物的混合物。 第一聚合物包括丙烯酸甲酯或丙烯酸乙酯残基的量为第一聚合物的约15重量%至约25重量%,马来酸酐残基的量为第一聚合物的约2重量%至约3.5重量%,以及 乙烯残基。 第二聚合物包括按第二聚合物的重量计约5%至约10%的量的丙烯酸丁酯残基,第二聚合物重量的约3%至约4%的马来酸酐残基和乙烯残基。 混合物中第一聚合物的量为约60重量%至约90重量%。 该混合物可进一步包括颜料-LDPE组合物,其中混合物中第一聚合物的量为约50%至约70%重量。

    INKJET RECORDING MEDIUM
    7.
    发明申请
    INKJET RECORDING MEDIUM 有权
    喷墨记录介质

    公开(公告)号:US20120194625A1

    公开(公告)日:2012-08-02

    申请号:US13017624

    申请日:2011-01-31

    CPC分类号: B41M5/5218

    摘要: An inkjet recording medium includes a substrate, a base layer disposed on the substrate, and an ink receiving layer disposed on the base layer. The ink receiving layer includes cationically-modified fumed silica having nanoparticles of alumina and/or silica mixed therein. The alumina nanoparticles have an individual particle size ranging from about 15 nm to about 50 nm, and the silica nanoparticles have an individual particle size ranging from about 5 nm to about 45 nm.

    摘要翻译: 喷墨记录介质包括基板,设置在基板上的基底层和设置在基底层上的墨接受层。 油墨接收层包括具有混合在其中的氧化铝和/或二氧化硅纳米颗粒的阳离子改性的热解法二氧化硅。 氧化铝纳米颗粒具有约15nm至约50nm的单独粒度,并且二氧化硅纳米颗粒具有约5nm至约45nm的单独粒度。

    Inkjet recording medium
    8.
    发明授权
    Inkjet recording medium 有权
    喷墨记录介质

    公开(公告)号:US08398233B2

    公开(公告)日:2013-03-19

    申请号:US13017624

    申请日:2011-01-31

    IPC分类号: B41J2/01

    CPC分类号: B41M5/5218

    摘要: An inkjet recording medium includes a substrate, a base layer disposed on the substrate, and an ink receiving layer disposed on the base layer. The ink receiving layer includes cationically-modified fumed silica having nanoparticles of alumina and/or silica mixed therein. The alumina nanoparticles have an individual particle size ranging from about 15 nm to about 50 nm, and the silica nanoparticles have an individual particle size ranging from about 5 nm to about 45 nm.

    摘要翻译: 喷墨记录介质包括基板,设置在基板上的基底层和设置在基底层上的墨接受层。 油墨接收层包括具有混合在其中的氧化铝和/或二氧化硅纳米颗粒的阳离子改性的热解法二氧化硅。 氧化铝纳米颗粒具有约15nm至约50nm的单独粒度,并且二氧化硅纳米颗粒具有约5nm至约45nm的单独粒度。