1.
公开(公告)号:US20230174740A1
公开(公告)日:2023-06-08
申请号:US18073854
申请日:2022-12-02
Applicant: Borealis AG
Inventor: Thomas Gkourmpis , Roland Kadar , Georgia Manika , Athanasios Theodoridis
CPC classification number: C08K3/04 , C08K3/042 , C08K3/041 , C08F10/06 , C08F10/02 , H01B1/24 , B32B27/32 , C08K2201/001 , C08K2201/014 , H01B9/027
Abstract: The invention relates to a semiconductive polyolefin composition comprising, (A) 80 to 99.5 wt. % of an olefin polymer base resin based on the total weight of the semiconductive polyolefin composition; (B) 0.1 to 10.0 wt. % of first carbonaceous structures based on the total weight of the semiconductive polyolefin composition; (C) 0.2 to 15.0 wt. % of carbon black and/or second carbonaceous structures based on the total weight of the semiconductive polyolefin composition; and (D) optionally additives; wherein the combined amount of components (B) and (C) is at least 0.3 wt. % and not more than 15.0 wt. % based on the total weight of the semiconductive polyolefin composition; and wherein the semiconductive polyolefin composition has an electrical percolation threshold of not more than 5 wt. % of the combined amount of components (B) and (C) dispersed in the olefin polymer base resin (A), the electrical percolation threshold being defined as the critical concentration in wt. % of the components (B) and (C) in the olefin polymer base resin (A) where an exponential increase in electrical conductivity is observed; wherein the polyolefin composition has a conductivity of at least 1·10−7 S/cm determined according to Broadband Dielectric Spectroscopy for a percolation threshold of 1.0 wt. % or lower and 2-point electrical measurements for a percolation threshold of more than 1.0 wt. %; and wherein components (A) to (D) add up to 100 wt. %.