Abstract: Polyolefin (PO) compositions derived from post-consumer recyclate (PCR) PO based materials having well balanced properties with regards to electric conductivity, impact performance, stiffness, and workability.
-
2.
公开(公告)号:US20240059883A1
公开(公告)日:2024-02-22
申请号:US18266981
申请日:2022-01-27
Applicant: Borealis AG
Inventor: Susanne Margarete Kahlen , Hermann Braun , Andreas Rössler-Czermak , Giovanni Federico Benedetti , Philip Knapen
IPC: C08L23/12
CPC classification number: C08L23/12 , C08L2205/025 , C08L2205/035 , C08L2207/20 , C08L2207/02
Abstract: Provided is a polyolefin composition including a) at least one heterophasic polypropylene copolymer with a melt flow rate MFR2 (230° C., 2.16 kg, measured according to ISO 1133) of at least 40 g/10 min, preferably of at least 60 g/10 min ; b) at least one polypropylene homopolymer with a melt flow rate MFR2 (230° C., 2.16 kg, measured according to ISO 1133) of at least 400 g/10 min; and c) a blend (A) of recycled plastic material comprising polypropylene and polyethylene in a ratio between 3:7 and 12:1, which is recovered from a waste plastic material derived from post-consumer and/or post-industrial waste with a melt flow rate MFR2 (230° C., 2.16 kg, measured according to ISO 1133) of at least 5 g/10 min. The polyolefin composition has a melt flow rate MFR2 (230° C., 2.16 kg, measured according to ISO 1133) of at least 20 g/10 min.
-