POLYPROPYLENE POLYETHYLENE MIXTURE UPGRADING

    公开(公告)号:US20230279208A1

    公开(公告)日:2023-09-07

    申请号:US18014185

    申请日:2021-07-05

    Applicant: Borealis AG

    Abstract: Use of a compatibilizer (B) for upgrading a polypropylene-polyethylene blend (A) comprising (A-1) polypropylene and (A-2) polyethylene wherein the weight ratio of polypropylene (A-1) to polyethylene (A-2) is in the range from 19:1 to 1:19 with respect to at least one or more of the following properties (i) elongation at break (ISO 527-1,2; F3/4), (ii) Charpy notched impact strength (1eA) (non-instrumented, ISO 179-1 at +23° C.), (iii) Charpy notched impact strength (1eA) (non-instrumented, ISO 179-1 at 0° C.), (iv) Charpy notched impact strength (1eA) (non-instrumented, ISO 179-1 at −20° C.), (v) puncture resistance (energy, IS07785-2 at +23° C.) and (vi) low temperature puncture resistance (energy, ISO 7765-2 at 0° C. or −20° C.), wherein compatibilizer (B) is used in an amount of 1 to 35 wt.-% preferably 2 to 25 wt.-%, more preferably 3 to 9 wt.-% with respect to the final composition.

    VISBREAKING PROCESS
    10.
    发明申请

    公开(公告)号:US20210024789A1

    公开(公告)日:2021-01-28

    申请号:US17012665

    申请日:2020-09-04

    Applicant: BOREALIS AG

    Abstract: A process for increasing MFR2 of a polyethylene copolymer or an ethylene plastomer or elastomer comprising: (I) extruding a copolymer of polyethylene copolymer having a density of 910 to 970 kg/m3 and an MFR2 of 1 and 100 g/10 min or an ethylene plastomer or elastomer having a density of 855 to 910 kg/m3 and an MFR2 of 0.5 and 100 g/10 min in the presence of 0.1 to 2 wt % of a non-peroxide radical initiator so as to produce a polyethylene copolymer having an MFR2 of 200 g/10 min or more, or an ethylene plastomer or elastomer having a MFR2 of 200 g/10 min or more.

Patent Agency Ranking