公开(公告)号:US20170225440A1
公开(公告)日:2017-08-10
申请号:US15453393
申请日:2017-03-08
Applicant: Chevron Phillips Chemical Company LP
Inventor: Mark L. HLAVINKA , Charles D. MILLS , Qing YANG , Guylaine ST. JEAN
CPC classification number: B32B27/327 , B32B27/08 , B32B27/32 , B32B2250/03 , B32B2250/242 , B32B2307/724 , B32B2439/70 , B32B2553/00 , G01D5/35316 , G01K11/3206 , G01L1/246 , G02B6/02204 , G02B6/29353 , Y10T428/31855
Abstract: A multilayer polymer film comprising an outer skin layer, an inner seal layer and at least one core layer disposed between the inner and outer skin layer, wherein the outer skin layers comprises a metallocene-catalyzed ethylene polymer having a density of equal to or greater than about 0.945 g/cc and a melt index equal to or greater than 0.5 g/10 min. A multilayer polymer film comprising a metallocene-catalyzed high-density polyethylene homopolymer skin layer and at least one core layer comprising a high-density polyethylene having a melt index of less than or equal to 2.0 g/10 min. A multilayer polymer film comprising at least a skin layer and a core layer wherein the skin layer comprises a metallocene-catalyzed ethylene polymer provided from a catalyst composition comprising a single metallocene and an activator support.
-
2.
公开(公告)号:US20140212607A1
公开(公告)日:2014-07-31
申请号:US13753132
申请日:2013-01-29
Applicant: CHEVRON PHILLIPS CHEMICAL COMPANY LP
Inventor: Jim H. ADDCOX , Guylaine ST. JEAN
IPC: C08L23/06
CPC classification number: C08L23/06 , A61F13/51462 , C08J5/18 , C08J2323/04 , C08J2491/06 , C08L23/04 , C08L23/08 , C08L91/06 , C08L2203/16 , Y10T428/1324
Abstract: A composition comprising a polymer and a wax wherein the polymer has a melt index of from about 0.5 g/10 min to about 4 g/10 min, a density of equal to or greater than about 0.945 g/cc which when formed into a film displays a moisture vapor transmission rate of less than about 0.55 g-mil/100 in2 in 24 hours as determined in accordance with ASTM F 1249.
Abstract translation: 包含聚合物和蜡的组合物,其中所述聚合物的熔体指数为约0.5g / 10min至约4g / 10min,密度等于或大于约0.945g / cc,当其形成膜时 在按照ASTM F1249测定的24小时内显示小于约0.55g / mil / 100in2的水蒸气透过率。
-
公开(公告)号:US20180057618A1
公开(公告)日:2018-03-01
申请号:US15805982
申请日:2017-11-07
Applicant: Chevron Phillips Chemical Company LP
Inventor: Ashish M. SUKHADIA , Guylaine ST. JEAN , Qing YANG , Max P. MCDANIEL
CPC classification number: C08F10/02 , C08F10/04 , C08F10/06 , C08F10/08 , C08F10/10 , C08F10/14 , C08J5/18 , C08J2323/08 , C08L23/0815 , C08L2203/16 , C08L2205/025
Abstract: An ethylene alpha-olefin copolymer having (a) a density of from about 0.910 g/cc to about 0.940 g/cc; (b) a weight average molecular weight of from about 150,000 g/mol to about 300,000 g/mol; and (c) a melt index at a load of 2.16 kg of from about 0.01 dg/10 min. to about 0.5 dg/min.; wherein a 1 mil blown film formed from the polymer composition is characterized by (i) a Dart Impact strength greater than about 175 g/mil; (ii) an Elmendorf machine direction tear strength greater than about 20 g/mil; and (iii) an Elmendorf transverse direction tear strength greater than about 475 g/mil.
-
公开(公告)号:US20210024671A1
公开(公告)日:2021-01-28
申请号:US17068486
申请日:2020-10-12
Applicant: Chevron Phillips Chemical Company LP
Inventor: Ashish M. SUKHADIA , Guylaine ST. JEAN , Qing YANG , Max P. MCDANIEL
IPC: C08F210/16 , C08F10/02 , C08F10/08 , C08F10/14 , C08J5/18 , C08L23/08 , C08F210/18 , C08F210/02
Abstract: An ethylene alpha-olefin copolymer having (a) a density of from about 0.910 g/cc to about 0.940 g/cc; (b) a weight average molecular weight of from about 150,000 g/mol to about 300,000 g/mol; and (c) a melt index at a load of 2.16 kg of from about 0.01 dg/10 min. to about 0.5 dg/min.; wherein a 1 mil blown film formed from the polymer composition is characterized by (i) a Dart Impact strength greater than about 175 g/mil; (ii) an Elmendorf machine direction tear strength greater than about 20 g/mil; and (iii) an Elmendorf transverse direction tear strength greater than about 475 g/mil.
-
公开(公告)号:US20140256901A1
公开(公告)日:2014-09-11
申请号:US13794052
申请日:2013-03-11
Applicant: CHEVRON PHILLIPS CHEMICAL COMPANY LP
Inventor: Ashish M. SUKHADIA , Guylaine ST. JEAN , Qing YANG , Max P. MCDANIEL
CPC classification number: C08F10/02 , C08F10/04 , C08F10/06 , C08F10/08 , C08F10/10 , C08F10/14 , C08J5/18 , C08J2323/08 , C08L23/0815 , C08L2203/16 , C08L2205/025
Abstract: An ethylene alpha-olefin copolymer having (a) a density of from about 0.910 g/cc to about 0.940 g/cc; (b) a weight average molecular weight of from about 150,000 g/mol to about 300,000 g/mol; and (c) a melt index at a load of 2.16 kg of from about 0.01 dg/10 min. to about 0.5 dg/min.; wherein a 1 mil blown film formed from the polymer composition is characterized by (i) a Dart Impact strength greater than about 175 g/mil; (ii) an Elmendorf machine direction tear strength greater than about 20 g/mil; and (iii) an Elmendorf transverse direction tear strength greater than about 475 g/mil.