    Abstract: Glass-ceramics exhibiting a Vickers indentation crack initiation threshold of at least 15 kgf are disclosed. These glass-ceramics may be ion exchangeable or ion exchanged. The glass-ceramics include a crystalline and amorphous phases generated by subjecting a thin precursor glass article to ceramming cycle having an average cooling rate in the range from about 10° C./minute to about 25° C./minute. In one or more embodiments, the crystalline phase may comprise at least 20 wt % of the glass-ceramics. The glass-ceramics may include β-spodumene ss as the predominant crystalline phase and may exhibit an opacity ≧about 85% over the wavelength range of 400-700 nm for an about 0.8 mm thickness and colors an observer angle of 10° and a CIE illuminant F02 determined with specular reflectance included of a* between −3 and +3, b* between −6 and +6, and L* between 88 and 97.

    Abstract translation: 公开了具有至少15kgf的维氏体压痕裂纹起始阈值的玻璃陶瓷。 这些玻璃陶瓷可以是离子交换的或离子交换的。 玻璃陶瓷包括通过使薄的前体玻璃制品经受平均冷却速率在约10℃/分钟至约25℃/分钟范围内的陶瓷循环而产生的结晶和非晶相。 在一个或多个实施方案中,结晶相可以包含至少20wt%的玻璃陶瓷。 玻璃陶瓷可以包括作为主要结晶相的聚硅氧烷树脂ss,并且在400-700nm的波长范围内可以显示大约85%的不透明度约0.8mm厚度,并且观察角度为10°,并且 CIE光源F02由包括-3和+3之间的a *,-6和+6之间的b *,以及88和97之间的L *决定。

Patent Agency Ranking