公开(公告)号:US12098466B2
公开(公告)日:2024-09-24
申请号:US18180318
申请日:2023-03-08
Applicant: Caterpillar Inc.
Inventor: Michael A. Pershing , Curtis A. Henning , Robert J. Pickerill , Scott A. Johnston
CPC classification number: C23C8/22 , C21D9/46 , C22C38/02 , C22C38/04 , C22C38/44 , C22C38/48 , C21D2211/001 , C21D2211/008 , C22C2204/00
Abstract: A carburized steel component, comprising a steel base including, by weight percent, from 0.08% to 0.35% carbon, 0.5% to 1.3% manganese, 0% to 0.35% silicon, 0.2% to 2.0% chromium, 0% to 4% nickel, 0% to 0.50% molybdenum, 0% to 0.06% niobium, and a remaining weight percent of iron, and a carburized layer of above 0.35% by weight carbon from a surface of the carburized layer to a carburized layer depth, wherein the carburized layer depth is from 0.5 mm to 3.0 mm, wherein the carburized layer comprises a microstructure including martensite, retained austenite, carbide, and less than 2% by volume non-martensitic transformation products (NMTP), and wherein the carburized layer includes a prior austenite average grain size of 3.0-8.0 microns from the surface to a depth of at least 0.2 mm.
-
公开(公告)号:US11624106B2
公开(公告)日:2023-04-11
申请号:US16822753
申请日:2020-03-18
Applicant: Caterpillar Inc.
Inventor: Michael A. Pershing , Curtis A. Henning , Robert J. Pickerill , Scott A. Johnston
Abstract: A carburized steel component, comprising a steel base including, by weight percent, from 0.08% to 0.35% carbon, 0.5% to 1.3% manganese, 0% to 0.35% silicon, 0.2% to 2.0% chromium, 0% to 4% nickel, 0% to 0.50% molybdenum, 0% to 0.06% niobium, and a remaining weight percent of iron, and a carburized layer of above 0.35% by weight carbon from a surface of the carburized layer to a carburized layer depth, wherein the carburized layer depth is from 0.5 mm to 3.0 mm, wherein the carburized layer comprises a microstructure including martensite, retained austenite, carbide, and less than 2% by volume non-martensitic transformation products (NMTP), and wherein the carburized layer includes a prior austenite average grain size of 3.0-8.0 microns from the surface to a depth of at least 0.2 mm.
-
公开(公告)号:US20180223411A1
公开(公告)日:2018-08-09
申请号:US15947893
申请日:2018-04-09
Applicant: Caterpillar Inc.
Inventor: Zachary S. Birky , Michael A. Pershing , Thomas E. Clements
IPC: C23C8/26 , C23C8/38 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/24 , C22C38/44 , C22C38/46 , C22C38/50 , C22C38/56 , C22C38/22 , C22C38/42
CPC classification number: C23C8/26 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/22 , C22C38/24 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/50 , C22C38/56 , C23C8/38
Abstract: A disclosure is directed to a method for rapidly nitriding steel, the method including: placing the steel in a furnace having an atmosphere comprising partially dissociated ammonia gas; heating the steel to a highest temperature in a range of 400 to 600° C. while holding a nitriding potential below 15 atm−1/2 during heat-up from 400° C. up to the highest temperature; and holding the steel at the highest temperature while continuing to maintain the nitriding potential below 15 atm−1/2, where a total time taken for the heating and holding the steel in the range of 400 to 600° C. during the nitriding is 15 hours or less, and where a composition of the steel comprises at least one of the group consisting of Al, Cr, Mo, V, and Ti.
-
公开(公告)号:US20160130692A1
公开(公告)日:2016-05-12
申请号:US14934569
申请日:2015-11-06
Applicant: Caterpillar Inc.
Inventor: Zachary S. Birky , Michael A. Pershing , Thomas E. Clements
IPC: C23C8/26 , C22C38/56 , C22C38/50 , C22C38/46 , C22C38/02 , C22C38/42 , C22C38/24 , C22C38/06 , C22C38/04 , C22C38/22 , C22C38/44
CPC classification number: C23C8/26 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/22 , C22C38/24 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/50 , C22C38/56 , C23C8/38
Abstract: A disclosure is directed to a method for rapidly nitriding steel, the method including: placing the steel in a furnace having an atmosphere comprising partially dissociated ammonia gas; heating the steel to a highest temperature in a range of 400 to 600° C. while holding a nitriding potential below 15 atm−1/2 during heat-up from 400° C. up to the highest temperature; and holding the steel at the highest temperature while continuing to maintain the nitriding potential below 15 atm−1/2, where a total time taken for the heating and holding the steel in the range of 400 to 600° C. during the nitriding is 15 hours or less, and where a composition of the steel comprises at least one of the group consisting of Al, Cr, Mo, V, and Ti.
Abstract translation: 本发明涉及一种用于快速氮化氮化的方法,该方法包括:将钢放置在具有包含部分解离的氨气的气氛的炉中; 在400〜600℃的范围内将钢加热至最高温度,同时在400℃升温至最高温度的同时保持氮化电位低于15atm-1/2; 并将钢保持在最高温度,同时继续保持渗氮电位低于15atm-1/2,其中在氮化期间加热和保持钢在400至600℃范围内的总时间为15 小时以下,钢的成分含有Al,Cr,Mo,V,Ti中的至少一种。
-
-
-