1.
公开(公告)号:US12275809B2
公开(公告)日:2025-04-15
申请号:US18487175
申请日:2023-10-16
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Yongwoo Inn , Alfred E. Brown, Jr. , Brandy Rutledge-Ryal , Carlos A. Cruz , Jay M. Chaffin
IPC: C08F210/16 , C08F4/6592 , C08F210/02 , C08L23/0807
Abstract: Ethylene-based polymers having a density of 0.952 to 0.968 g/cm3, a ratio of HLMI/MI from 185 to 550, an IB parameter from 1.46 to 1.80, a tan δ at 0.1 sec−1 from 1.05 to 1.75 degrees, and a slope of a plot of viscosity versus shear rate at 100 sec−1 from 0.18 to 0.28 are described, with low melt flow versions having a HLMI from 10 to 30 g/10 min and a Mw from 250,000 to 450,000 g/mol, and high melt flow versions having a HLMI from 30 to 55 g/10 min and a Mw from 200,000 to 300,000 g/mol. These polymers have the processability of chromium-based resins, but with improved stress crack resistance and topload strength for bottles and other blow molded products.
-
公开(公告)号:US20210024728A1
公开(公告)日:2021-01-28
申请号:US16522788
申请日:2019-07-26
Applicant: Chevron Phillips Chemical Company LP
Inventor: Carlos A. Cruz , Yongwoo Inn , Justin Lumbley , Brandy Rutledge-Ryal , John R. Rathman , Jennifer L. Hicks , Jay M. Chaffin
IPC: C08L23/08 , C08F210/16 , C08F4/6592 , C08K3/08
Abstract: Ethylene-based polymers having a density of 0.952 to 0.965 g/cm3, a high load melt index (HLMI) from 5 to 25 g/10 min, a weight-average molecular weight from 275,000 to 450,000 g/mol, a number-average molecular weight from 15,000 to 40,000 g/mol, a viscosity at HLMI from 1400 to 4000 Pa-sec, and a tangent delta at 0.1 sec−1 from 0.65 to 0.98 degrees. These polymers have the processability of chromium-based resins, but with improved stress crack resistance, and can be used in large-part blow molding applications.
-
3.
公开(公告)号:US20230124846A1
公开(公告)日:2023-04-20
申请号:US18062091
申请日:2022-12-06
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Yongwoo Inn , Alfred E. Brown, JR. , Brandy Rutledge-Ryal , Carlos A. Cruz , Jay M. Chaffin
IPC: C08F210/02 , C08F210/16 , C08L23/08
Abstract: Ethylene-based polymers having a density of 0.952 to 0.968 g/cm3. a ratio of HLMI/MI from 185 to 550. an IB parameter from 1.46 to 1.80, a tan δ at 0.1 sec-1 from 1.05 to 1.75 degrees, and a slope of a plot of viscosity versus shear rate at 100 sec-1 from 0.18 to 0.28 are described, with low melt flow versions having a HLMI from 10 to 30 g/10 min and a Mw from 250,000 to 450,000 g/mol, and high melt flow versions having a HLMI from 30 to 55 g/10 min and a Mw from 200,000 to 300,000 g/mol. These polymers have the processability of chromium-based resins, but with improved stress crack resistance and topload strength for bottles and other blow molded products.
-
4.
公开(公告)号:US20230019739A1
公开(公告)日:2023-01-19
申请号:US17935612
申请日:2022-09-27
Applicant: Chevron Phillips Chemical Company LP
Inventor: Carlos A. Cruz , Yongwoo Inn , John R. Rathman , Youlu Yu , Ashish M. Sukhadia , Jay M. Chaffin
IPC: C08F210/02 , C08K5/14
Abstract: Ethylene-based polymers are generally characterized by a high load melt index of less than 12 g/10 min, a weight-average molecular weight from 200,000 to 550,000 g/mol, a number-average molecular weight from 18,000 to 48,000 g/mol, a CY-a parameter of less than 0.12, a tan δ at 0.1 sec-1 from 0.5 to 0.9 degrees, a tan δ at 100 sec-1 from 0.5 to 0.75 degrees, and a viscosity at 0.001 sec-1 from 1.3 x 106 to 1 x 107 Pa-sec. These ethylene polymers can be produced by peroxide-treating a bimodal molecular weight distribution dual metallocene-catalyzed resin, and can be used to produce blow molded bottles and other blow molded products.
-
公开(公告)号:US12234348B2
公开(公告)日:2025-02-25
申请号:US17745962
申请日:2022-05-17
Applicant: Chevron Phillips Chemical Company LP
Inventor: Carlos A. Cruz , Yongwoo Inn , Justin Lumbley , Brandy Rutledge-Ryal , John R. Rathman , Jennifer L Hicks , Jay M. Chaffin
IPC: C08F210/16 , C08F4/6592 , C08K3/08 , C08L23/0807
Abstract: Ethylene-based polymers having a density of 0.952 to 0.965 g/cm3, a high load melt index (HLMI) from 5 to 25 g/10 min, a weight-average molecular weight from 275,000 to 450,000 g/mol, a number-average molecular weight from 15,000 to 40,000 g/mol, a viscosity at HLMI from 1400 to 4000 Pa-sec, and a tangent delta at 0.1 sec−1 from 0.65 to 0.98 degrees. These polymers have the processability of chromium-based resins, but with improved stress crack resistance, and can be used in large-part blow molding applications.
-
6.
公开(公告)号:US11505630B2
公开(公告)日:2022-11-22
申请号:US17200976
申请日:2021-03-15
Applicant: Chevron Phillips Chemical Company LP
Inventor: Carlos A. Cruz , Yongwoo Inn , John R. Rathman , Youlu Yu , Ashish M. Sukhadia , Jay M. Chaffin
IPC: C08F10/02 , C08F210/16 , C08F210/02 , C08K5/14
Abstract: Ethylene-based polymers are generally characterized by a high load melt index of less than 12 g/10 min, a weight-average molecular weight from 200,000 to 550,000 g/mol, a number-average molecular weight from 18,000 to 48,000 g/mol, a CY-a parameter of less than 0.12, a tan δ at 0.1 sec−1 from 0.5 to 0.9 degrees, a tan δ at 100 sec−1 from 0.5 to 0.75 degrees, and a viscosity at 0.001 sec−1 from 1.3×106 to 1×107 Pa-sec. These ethylene polymers can be produced by peroxide-treating a bimodal molecular weight distribution dual metallocene-catalyzed resin, and can be used to produce blow molded bottles and other blow molded products.
-
7.
公开(公告)号:US20220119562A1
公开(公告)日:2022-04-21
申请号:US17074784
申请日:2020-10-20
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Yongwoo Inn , Alfred E. Brown, JR. , Brandy Rutledge-Ryal , Carlos A. Cruz , Jay M. Chaffin
IPC: C08F210/02
Abstract: Ethylene-based polymers having a density of 0.952 to 0.968 g/cm3, a ratio of HLMI/MI from 185 to 550, an IB parameter from 1.46 to 1.80, a tan δ at 0.1 sec−1 from 1.05 to 1.75 degrees, and a slope of a plot of viscosity versus shear rate at 100 sec−1 from 0.18 to 0.28 are described, with low melt flow versions having a HLMI from 10 to 30 g/10 min and a Mw from 250,000 to 450,000 g/mol, and high melt flow versions having a HLMI from 30 to 55 g/10 min and a Mw from 200,000 to 300,000 g/mol. These polymers have the processability of chromium-based resins, but with improved stress crack resistance and topload strength for bottles and other blow molded products.
-
8.
公开(公告)号:US20240052073A1
公开(公告)日:2024-02-15
申请号:US18487175
申请日:2023-10-16
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Yongwoo Inn , Alfred E. Brown, JR. , Brandy Rutledge-Ryal , Carlos A. Cruz , Jay M. Chaffin
IPC: C08F210/02 , C08F210/16 , C08L23/08
CPC classification number: C08F210/02 , C08F210/16 , C08L23/0815 , C08F2420/01 , C08F2420/03 , C08F4/65925
Abstract: Ethylene-based polymers having a density of 0.952 to 0.968 g/cm3, a ratio of HLMI/MI from 185 to 550, an IB parameter from 1.46 to 1.80, a tan δ at 0.1 sec−1 from 1.05 to 1.75 degrees, and a slope of a plot of viscosity versus shear rate at 100 sec−1 from 0.18 to 0.28 are described, with low melt flow versions having a HLMI from 10 to 30 g/10 min and a Mw from 250,000 to 450,000 g/mol, and high melt flow versions having a HLMI from 30 to 55 g/10 min and a Mw from 200,000 to 300,000 g/mol. These polymers have the processability of chromium-based resins, but with improved stress crack resistance and topload strength for bottles and other blow molded products.
-
9.
公开(公告)号:US11866529B2
公开(公告)日:2024-01-09
申请号:US18062091
申请日:2022-12-06
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Yongwoo Inn , Alfred E. Brown, Jr. , Brandy Rutledge-Ryal , Carlos A. Cruz , Jay M. Chaffin
IPC: C08L23/08 , C08F210/16 , C08F4/653 , C08F4/6592 , C08F210/02
CPC classification number: C08F210/02 , C08F210/16 , C08L23/0815 , C08F4/65925 , C08F4/65927 , C08F2420/01 , C08F2420/03
Abstract: Ethylene-based polymers having a density of 0.952 to 0.968 g/cm3, a ratio of HLMI/MI from 185 to 550, an IB parameter from 1.46 to 1.80, a tan δ at 0.1 sec−1 from 1.05 to 1.75 degrees, and a slope of a plot of viscosity versus shear rate at 100 sec−1 from 0.18 to 0.28 are described, with low melt flow versions having a HLMI from 10 to 30 g/10 min and a Mw from 250,000 to 450,000 g/mol, and high melt flow versions having a HLMI from 30 to 55 g/10 min and a Mw from 200,000 to 300,000 g/mol. These polymers have the processability of chromium-based resins, but with improved stress crack resistance and topload strength for bottles and other blow molded products.
-
10.
公开(公告)号:US11814455B2
公开(公告)日:2023-11-14
申请号:US17935612
申请日:2022-09-27
Applicant: Chevron Phillips Chemical Company LP
Inventor: Carlos A. Cruz , Yongwoo Inn , John R. Rathman , Youlu Yu , Ashish M. Sukhadia , Jay M. Chaffin
IPC: C08F210/02 , C08F210/16 , C08K5/14 , C08F10/02
CPC classification number: C08F210/02 , C08K5/14 , C08F10/02 , C08F210/16 , C08F10/02 , C08F2810/10
Abstract: Ethylene-based polymers are generally characterized by a high load melt index of less than 12 g/10 min, a weight-average molecular weight from 200,000 to 550,000 g/mol, a number-average molecular weight from 18,000 to 48,000 g/mol, a CY-a parameter of less than 0.12, a tan δ at 0.1 sec−1 from 0.5 to 0.9 degrees, a tan δ at 100 sec−1 from 0.5 to 0.75 degrees, and a viscosity at 0.001 sec−1 from 1.3×106 to 1×107 Pa-sec. These ethylene polymers can be produced by peroxide-treating a bimodal molecular weight distribution dual metallocene-catalyzed resin, and can be used to produce blow molded bottles and other blow molded products.
-
-
-
-
-
-
-
-
-