PELLETS OF LIGHTLY VIS-BROKEN POLYPROPYLENE
    7.
    发明申请
    PELLETS OF LIGHTLY VIS-BROKEN POLYPROPYLENE 审中-公开
    轻质VIS-BROKEN聚丙烯薄膜

    公开(公告)号:US20170051118A1

    公开(公告)日:2017-02-23

    申请号:US14832350

    申请日:2015-08-21

    IPC分类号: C08J5/00 C08F110/06 C08J3/24

    摘要: A process including vis-breaking of polypropylene in the presence of 3,6,9-triethyl-3,6,9-trimethyl-1,4,7-triperoxonane to obtain vis-broken polypropylene is provided. The vis-broken polypropylene may be pelletized to obtain pellets. A ratio of a melt flow rate (MI2) of the pellets to a melt flow rate (MI2) of the polypropylene prior to the vis-breaking may be greater than 1:1 and at most 4:1. The pellets may be used to form articles.

    摘要翻译: 提供了一种包括在3,6,9-三乙基-3,6,9-三甲基-1,4,7-三过氧苯甲酸存在下的聚丙烯的断裂以获得可折断的聚丙烯的方法。 可以将可见光聚丙烯造粒以获得颗粒。 颗粒之间的熔体流动速率(MI2)与破坏前的聚丙烯的熔体流动速率(MI2)之比可以大于1:1,最多为4:1。 颗粒可用于形成制品。

    PROPYLENE-BASED POLYMER WITH REDUCED HIGH-MOLECULAR WEIGHT PORTION
    8.
    发明申请
    PROPYLENE-BASED POLYMER WITH REDUCED HIGH-MOLECULAR WEIGHT PORTION 有权
    具有降低高分子重量份的丙烯聚合物

    公开(公告)号:US20160280812A1

    公开(公告)日:2016-09-29

    申请号:US15035649

    申请日:2014-11-14

    IPC分类号: C08F10/06

    摘要: The present disclosure provides a process for producing propylene-based polymer. The process includes contacting, under polymerization conditions in a gas phase polymerization reactor, propylene monomer and optionally one or more comonomers with a Ziegler-Natta catalyst composition. The process includes maintaining the temperature of a reaction zone of the reactor at a temperature from greater than 72° C. to less than or equal to 85° C., and forming a propylene-based polymer having a molecular weight (Mw) greater than 100,000, and a Mz+1/Mz less than 2.20. The resultant propylene-based polymer is advantageous in fiber applications.

    摘要翻译: 本公开内容提供了一种生产基于丙烯的聚合物的方法。 该方法包括在气相聚合反应器中的聚合条件下使丙烯单体和任选的一种或多种共聚单体与齐格勒 - 纳塔催化剂组合物接触。 该方法包括将反应器的反应区的温度保持在大于72℃至小于或等于85℃的温度,并形成分子量(Mw)大于 100,000,Mz + 1 / Mz小于2.20。 得到的丙烯类聚合物在纤维应用中是有利的。