公开(公告)号:US20170073785A1
公开(公告)日:2017-03-16
申请号:US15123076
申请日:2015-03-03
发明人: Yuuki TANAKA , Makoto HARITANI , Takahiro MIYAZAKI , Kouji MORITA , Yoshihiro TANIMURA , Toshimasa ITO , Tadashi NISHIWAKI , Tomomitsu FUKUOKA
IPC分类号: C21D6/00 , C22C38/58 , C22C38/50 , C22C38/48 , C22C38/00 , C22C38/44 , C22C38/42 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/60 , C22C38/46
摘要: The present invention provides an age hardening type bainitic microalloyed steel having a composition which includes, in terms of mass %: 0.06-0.35% of C; 0.01-2.00% of Si; 0.10-3.00% of Mn; 0.001-0.200% of S; 0.001-2.00% of Cu; 0.40-3.00% of Ni; 0.10-3.00% of Cr; 0.10-1.00% of Mo; 0.10-1.00% of V; and 0.001-0.100% of s-Al, with the remainder being Fe and unavoidable impurities, and which satisfies a value of the following expression (1) to be 20 or larger and a value of the following expression (2) to be 0.82 or larger: 3×[C]+10×[Mn]+2×[Cu]+2×[Ni]+12×[Cr]+9×[Mo]+2×[V] expression (1); 1.66×[C]+0.18×[Si]+0.27×[Mn]+0.09×[Ni]+0.32×[Cr]+0.34×[Mo]+0.44×[V] expression (2), in which each [ ] in the expression (1) and the expression dicates a content of the element shown therein in terms of mass %.
摘要翻译: 其中表达式(1)中的每个[]和表达式以质量%表示其中所示的元素的含量。
-
2.
公开(公告)号:US20180245172A1
公开(公告)日:2018-08-30
申请号:US15558963
申请日:2016-03-16
发明人: Masato YUYA , Motoki TAKASUGA , Taizo MAKINO , Masashi HIGASHIDA , Tatsuya HASEGAWA , Kouji MORITA , Toshimasa ITO , Tomomitsu FUKUOKA , Tadashi NISHIWAKI , Yoshihiro TANIMURA
IPC分类号: C21D8/00 , C21D6/00 , C21D1/18 , C22C38/58 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/44 , C22C38/42 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00
CPC分类号: C21D8/005 , C21D1/18 , C21D6/004 , C21D6/005 , C21D6/008 , C21D6/02 , C21D8/065 , C21D9/0068 , C21D9/525 , C21D2211/002 , C22C38/001 , C22C38/002 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/20 , C22C38/22 , C22C38/24 , C22C38/38 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/58
摘要: Age hardenable steel is low in hardness after hot forging, providing a machine part with the desired fatigue strength and yield strength by aging treatment, and high in toughness after aging treatment, comprising C: 0.09 to 0.20%, Si: 0.01 to 0.40%, Mn: 1.5 to 2.5%, S: 0.001 to 0.045%, Cr: over 1.00% to 2.00%, Al: 0.001 to 0.060%, V: 0.22 to 0.55%, N: over 0.0080 to 0.0170%, and a balance of Fe and impurities, where an area rate of bainite structures is 80% or more, an effective V ratio (amount of dissolved V/total amount of V) is 0.9 or more, a P and Ti in the impurities is P: 0.03% or less and Ti: less than 0.005%, and the chemical composition is one where the following F1 is 1.00 or less and the F2 is 0.30 or more: F1=C+0.1×Si+0.2×Mn+0.15×Cr+0.35×V F2=−4.5×C+Mn+Cr−3.5×V
-