Product and process
    1.
    发明授权
    Product and process 失效
    产品和工艺

    公开(公告)号:US3878178A

    公开(公告)日:1975-04-15

    申请号:US35479273

    申请日:1973-04-26

    申请人: DU PONT

    CPC分类号: D02J1/228 D01F6/38

    摘要: This application discloses acrylic fibers having high tenacity, a break elongation of 8-18% and a shrinkage in boiling water of 13-26% in combination with an X-ray porosity index less than about 1.5 in the void size range of each of 45-90A and 90-140A and a molecular orientation of at least about 66.5, the particular fiber having the chemical composition of 93-95% acrylonitrile, 5-7% methylacrylate and up to 0.5% sodium styrene sulfonate. The fibers are prepared by specific drawing, drying and redrawing steps.

    摘要翻译: 本申请公开了具有高强度,断裂伸长率为8-18%,沸水收缩率为13-26%的丙烯酸纤维,以及在45度的空隙尺寸范围内的X射线孔隙率小于约1.5 -90A和90-140A,分子取向为至少约66.5,特定纤维的化学组成为93-95%丙烯腈,5-7%甲基丙烯酸酯和至多0.5%苯乙烯磺酸钠。 纤维通过特定的拉伸,干燥和再拉伸步骤制备。