    摘要: The firing shrinkage of ceramic film casting mixtures can be increased by adding a high molecular weight mixed ester or a mixture of various high molecular weight mixed esters to them. The ceramic material of the ceramic film casting mixtures is composed preferably of lead titanate, silicon carbide, silicon nitride, beryllium oxide or aluminum oxide. Preferably, the mixed esters are derived from at least one C.sub.2 -C.sub.10 -dicarboxylic acid and at least one C.sub.8 -C.sub.24 -monocarboxylic acid. The proportion of high molecular weight mixed ester in the film casting mixture amounts to up to 5% by weight, based on the proportion of solids in the casting mixture, including sintering aids.The process makes it possible to alter the composition of a slip and still use the old tools which require an unaltered firing shrinkage.

    摘要翻译: 可以通过向其中加入高分子量混合酯或各种高分子量混合酯的混合物来提高陶瓷膜浇铸混合物的焙烧收缩率。 陶瓷膜铸造混合物的陶瓷材料优选由钛酸铅,碳化硅,氮化硅,氧化铍或氧化铝组成。 优选地,混合酯衍生自至少一种C 2 -C 10 - 二羧酸和至少一种C 8 -C 24 - 一元羧酸。 基于浇铸混合物中固体比例(包括烧结助剂),薄膜浇注混合物中高分子量混合酯的比例达到5%(重量)。 该方法使得可以改变滑移的组成并且仍然使用需要不变的燃烧收缩的旧工具。