Low Alloy Steels With Superior Corrosion Resistance For Oil Country Tubular Goods
    1.
    发明申请
    Low Alloy Steels With Superior Corrosion Resistance For Oil Country Tubular Goods 有权
    低合金钢,具有优异的耐油腐蚀性,适用于石油国家管材

    公开(公告)号:US20110120723A1

    公开(公告)日:2011-05-26

    申请号:US12600949

    申请日:2008-05-02

    摘要: The present application describes a steel composition that provides enhanced corrosion resistance. This steel composition includes one of vanadium in an amount of 1 wt % to 9 wt %, titanium in an amount of about 1 wt % to 9 wt %, and a combination of vanadium and titanium in an amount of 1 wt % to about 9 wt %. In addition, the steel composition includes carbon in an amount of 0.03 wt % to about 0.45 wt %, manganese in an amount up to 2 wt % and silicon in an amount up to 0.45 wt %. In one embodiment, the steel composition includes a microstructure of one of the following: ferrite, martensite, tempered martensite, dual phase ferrite and martensite, and dual phase ferrite and tempered martensite. Further, the present application describes a method for processing the steel composition and use of equipment such as oil country tubular goods, fabricated with the steel composition.

    摘要翻译: 本申请描述了提供增强的耐腐蚀性的钢组合物。 该钢组合物包括1重量%至9重量%的钒中的一种,约1重量%至9重量%的钛,以及1重量%至约9重量%的钒和钛的组合 重量%。 此外,钢组合物包括0.03重量%至约0.45重量%的碳,最多达2重量%的锰和至多0.45重量%的硅。 在一个实施方案中,钢组合物包括以下之一的微结构:铁素体,马氏体,回火马氏体,双相铁素体和马氏体,以及双相铁素体和回火马氏体。 此外,本申请描述了用钢组合物制造的用于加工钢组合物和使用诸如油井筒状物品的设备的方法。

    Low alloy steels with superior corrosion resistance for oil country tubular goods
    2.
    发明授权
    Low alloy steels with superior corrosion resistance for oil country tubular goods 有权
    低合金钢,具有优异的耐油性能,适用于油井管状物品

    公开(公告)号:US08691030B2

    公开(公告)日:2014-04-08

    申请号:US12600949

    申请日:2008-05-02

    摘要: The present application describes a steel composition that provides enhanced corrosion resistance. This steel composition includes one of vanadium in an amount of 1 wt % to 9 wt %, titanium in an amount of about 1 wt % to 9 wt %, and a combination of vanadium and titanium in an amount of 1 wt % to about 9 wt %. In addition, the steel composition includes carbon in an amount of 0.03 wt % to about 0.45 wt %, manganese in an amount up to 2 wt % and silicon in an amount up to 0.45 wt %. In one embodiment, the steel composition includes a microstructure of one of the following: ferrite, martensite, tempered martensite, dual phase ferrite and martensite, and dual phase ferrite and tempered martensite. Further, the present application describes a method for processing the steel composition and use of equipment such as oil country tubular goods, fabricated with the steel composition.

    摘要翻译: 本申请描述了提供增强的耐腐蚀性的钢组合物。 该钢组合物包括1重量%至9重量%的钒中的一种,约1重量%至9重量%的钛,以及1重量%至约9重量%的钒和钛的组合 重量%。 此外,钢组合物包括0.03重量%至约0.45重量%的碳,最多达2重量%的锰和至多0.45重量%的硅。 在一个实施方案中,钢组合物包括以下之一的微结构:铁素体,马氏体,回火马氏体,双相铁素体和马氏体,以及双相铁素体和回火马氏体。 此外,本申请描述了用钢组合物制造的用于加工钢组合物和使用诸如油井筒状物品的设备的方法。

    Top of the Line Corrosion Apparatus
    3.
    发明申请
    Top of the Line Corrosion Apparatus 有权
    线腐蚀设备顶部

    公开(公告)号:US20100147056A1

    公开(公告)日:2010-06-17

    申请号:US12606781

    申请日:2009-10-27

    IPC分类号: G01N17/00

    CPC分类号: G01N17/002 G01N25/56

    摘要: The described invention relates to a method for determining corrosion in wet gas pipelines comprising: a) using a portion of the liquid phase from a wet gas pipeline; b) placing said portion in a high pressure, high temperature autoclave to prepare a saturated vapor phase; c) transferring the saturated vapor to a corrosion test unit, said unit having a specimen holder section having external, temperature adjustable means, and specimens being arranged in one or more positions within the specimen holder; d) chilling said specimen holder section so as to cause condensation onto said corrosion testing specimens; and, e) calculating a value selected from the group consisting of corrosions rate, pitting of the specimen, weight loss of the specimen, and any combination thereof. The invention process can be practiced in a separate laboratory apparatus designed to accomplish the above method, or in a similar online apparatus set up in a semi-batch mode or continuous mode.

    摘要翻译: 本发明涉及一种用于确定湿气管线腐蚀的方法,包括:a)使用来自湿气管道的一部分液相; b)将所述部分放置在高压高温高压釜中以制备饱和气相; c)将饱和蒸汽转移到腐蚀测试单元,所述单元具有具有外部温度可调节装置的样本保持器部分,并且样本被布置在样本保持器内的一个或多个位置; d)冷却所述试样保持器部分以使所述腐蚀试验样品冷凝; 以及e)计算从由腐蚀速率,试样的点蚀,试样的重量损失及其任何组合组成的组中选择的值。 本发明方法可以在设计用于实现上述方法的单独的实验室装置中或在以半批式或连续模式设置的类似在线装置中实施。

    Top of the line corrosion apparatus
    4.
    发明授权
    Top of the line corrosion apparatus 有权
    线腐蚀装置顶部

    公开(公告)号:US08261601B2

    公开(公告)日:2012-09-11

    申请号:US12606781

    申请日:2009-10-27

    IPC分类号: G01N17/00

    CPC分类号: G01N17/002 G01N25/56

    摘要: The described invention relates to a method for determining corrosion in wet gas pipelines comprising: a) using a portion of the liquid phase from a wet gas pipeline; b) placing said portion in a high pressure, high temperature autoclave to prepare a saturated vapor phase; c) transferring the saturated vapor to a corrosion test unit, said unit having a specimen holder section having external, temperature adjustable means, and specimens being arranged in one or more positions within the specimen holder; d) chilling said specimen holder section so as to cause condensation onto said corrosion testing specimens; and, e) calculating a value selected from the group consisting of corrosions rate, pitting of the specimen, weight loss of the specimen, and any combination thereof. The invention process can be practiced in a separate laboratory apparatus designed to accomplish the above method, or in a similar online apparatus set up in a semi-batch mode or continuous mode.

    摘要翻译: 本发明涉及一种用于确定湿气管线腐蚀的方法,包括:a)使用来自湿气管道的一部分液相; b)将所述部分放置在高压高温高压釜中以制备饱和气相; c)将饱和蒸汽转移到腐蚀测试单元,所述单元具有具有外部温度可调节装置的样本保持器部分,并且样本被布置在样本保持器内的一个或多个位置; d)冷却所述试样保持器部分以使所述腐蚀试验样品冷凝; 以及e)计算从由腐蚀速率,试样的点蚀,试样的重量损失及其任何组合组成的组中选择的值。 本发明方法可以在设计用于实现上述方法的单独的实验室装置中或在以半批式或连续模式设置的类似在线装置中实施。