Abstract: A method of making a material for capturing carbon dioxide from the earth's atmosphere, comprises producing an acid and a base with an electrochemical acid-base generator; dissolving a mineral in the acid to produce a mineral rich solution, separating silica from the mineral rich solution to form a silica depleted solution; adding a first portion of the base to the silica depleted solution to remove impurities by precipitation, adding a second portion of the base until ferrous hydroxide (Fe(OH)2) precipitates, then pausing base addition and removing the ferrous hydroxide precipitate from the solution. Then adding a third portion of the base to the iron-depleted solution to precipitate magnesium hydroxide (Mg(OH)2) and/or calcium hydroxide (Ca(OH)2). Then recovering a salt solution and directing the recovered salt solution to the electrochemical acid-base generator to
-
公开(公告)号:US20240425994A1
公开(公告)日:2024-12-26
申请号:US18825688
申请日:2024-09-05
Applicant: ELECTRASTEEL, INC.
Inventor: Ai Quoc PHAM , Sandeep NIJHAWAN , Kevin GALLOWAY , Adolfredo ALVAREZ , Philip WAGNER , Steven FATUR
IPC: C25B1/20 , C02F1/461 , C02F101/10 , C02F103/08 , C25B1/22 , C25B9/19 , C25B9/70 , C25B15/08
Abstract: A method of making a material for capturing carbon dioxide from the earth's atmosphere, comprises producing an acid and a base with an electrochemical acid-base generator; dissolving a mineral in the acid to produce a mineral rich solution, separating silica from the mineral rich solution to form a silica depleted solution; adding a first portion of the base to the silica depleted solution to remove impurities by precipitation, adding a second portion of the base until ferrous hydroxide (Fe(OH)2) precipitates, then pausing base addition and removing the ferrous hydroxide precipitate from the solution. Then adding a third portion of the base to the iron-depleted solution to precipitate magnesium hydroxide (Mg(OH)2) and/or calcium hydroxide (Ca(OH)2). Then recovering a salt solution and directing the recovered salt solution to the electrochemical acid-base generator to produce a new acid and a new base. The magnesium hydroxide and/or calcium hydroxide may be used to capture and sequester carbon dioxide from a CO2-containing gas (e.g., air) by forming a carbonate or from the ocean by forming bicarbonate.
-