Flux compositions for steel galvanization

    公开(公告)号:US10793940B2

    公开(公告)日:2020-10-06

    申请号:US14062170

    申请日:2013-10-24

    IPC分类号: C23C2/30 C23C2/02 C23C2/06

    摘要: A flux composition for treating a metal surface prior to batch hot galvanizing in molten zinc-based alloys is disclosed. The flux composition can include (a) 40 to 70 wt. % zinc chloride, (b) 10 to 30 wt. % ammonium chloride, (c) 6 to 30 wt. % of a set of at least two alkali or alkaline earth metal halides, (d) from 0.1 to 2 wt. % lead chloride, and (e) from 2 to 15 wt. % tin chloride, provided that the combined amounts of lead chloride and tin chloride represent at least 2.5 wt. % of the composition. A fluxing bath having this flux composition dissolved in water for use in galvanizing processes, as well as, a method for continuous or batch-wise treatment of metal articles in order to produce a protective coating layer with a thickness ranging from 5 to 30 μm is also disclosed.

    CONTINUOUS SINGLE-DIP PROCESS FOR GALVANIZATION OF STEEL LONG PRODUCTS INTO Zn-Al-Mg ALLOYS
    4.
    发明申请
    CONTINUOUS SINGLE-DIP PROCESS FOR GALVANIZATION OF STEEL LONG PRODUCTS INTO Zn-Al-Mg ALLOYS 审中-公开
    将钢产品长时间放入Zn-Al-Mg合金的连续单切工艺

    公开(公告)号:US20140120370A1

    公开(公告)日:2014-05-01

    申请号:US14062195

    申请日:2013-10-24

    IPC分类号: C23C2/36 B32B15/01

    摘要: By first fluxing a steel long product with novel specific flux compositions, it is possible to continuously produce, more uniform, smoother and void-free galvanized coatings on such steel long products in a single hot dip galvanization step making use of zinc-aluminum alloys or zinc-aluminum-magnesium alloys with less than 95 wt. % zinc. This is achieved by providing specific amounts of lead chloride and tin chloride in a flux composition comprising (a) more than 40 and less than 70 weight % zinc chloride, (b) from 10 to 30 weight % ammonium chloride, (c) more than 6 and less than 30 weight % of a set of at least two alkali or alkaline earth metal chlorides.

    摘要翻译: 通过首先使具有新型特定助焊剂组合物的长钢产品熔化,可以在单次热浸镀锌步骤中在这种钢制长产品上连续生产更均匀,更均匀,更平滑和无空隙的镀锌涂层,使用锌 - 铝合金或 小于95重量%的锌 - 铝 - 镁合金 %锌。 这通过在焊剂组合物中提供特定量的氯化铅和氯化锡来实现,所述助焊剂组合物包含(a)大于40重量%且小于70重量%的氯化锌,(b)10至30重量%的氯化铵,(c) 6和小于30重量%的一组至少两种碱金属或碱土金属氯化物。