摘要:
A fire resistant composition for forming a fire resistant ceramic at elevated temperatures, the composition comprising: at least 15% by weight based on the total weight of the composition of a polymer base composition comprising at least 50% by weight of an organic polymer; and at least 20% by weight based on the total weight of the composition of a silicate mineral filler; wherein upon exposure to an elevated temperature (experienced under fire conditions), the fire resistant composition is useful for passive fire protection applications, particularly cables, the fluxing oxide is present in an amount of from 1 to 15% by weight of the residue.
摘要:
A method for modifying a substrate containing a natural polymeric material to improve its interaction with other materials, the method comprising: A) Treating the substrate containing the natural polymeric material with a modifying agent selected from the group consisting of organo-functional coupling agents and multi-functional amine containing organic compounds; and B) optionally exposing the substrate containing natural polymeric material with one or more treatments selected from the group consisting of: i) subjecting the substrate to extraction with a solvent to reduce the content of extractable materials associated with the natural polymeric material prior to or during treatment with the modifying agent; ii) treatment with a physical field selected from static physical fields, high-frequency alternating physical fields and combinations of two or more thereof either prior to, during or after treatment with the modifying agent; and iii) oxidation of at least part of the natural polymeric material prior to or during treatment with the modifying agent.