公开(公告)号:US11318649B2
公开(公告)日:2022-05-03
申请号:US17104027
申请日:2020-11-25
Applicant: Heraeus Amloy Technologies GmbH
Inventor: Elena Bien , Hans Jurgen Wachter , Eugen Milke , Hamed Shakur Shahabi , Christian Pietsch
Abstract: One aspect relates to an injection molding system for the injection molding of amorphous metals, an injection molding unit for the injection molding of amorphous metals and an injection molding process for amorphous metals.
The injection molding system includes a channel for feeding a molten metal and a slider unit including a slider and a pressure system. The slider is located between the channel and at least one injection molding cavity and is movable between a rest position and an injection position. In the rest position, the slider blocks the access of the molten metal to the injection molding cavity and in the injection position it allows the molten metal to access the injection molding cavity. The pressure system holds the slider in the rest position and allows the slider to move to the injection position when a minimum pressure is exceeded.-
公开(公告)号:US20220161312A1
公开(公告)日:2022-05-26
申请号:US17433972
申请日:2020-02-24
Applicant: HERAEUS AMLOY TECHNOLOGIES GMBH
Inventor: Moritz Stolpe , Martin Schlott , Eugen Milke , Ralf Busch
Abstract: The invention relates to a method for producing a shaped part comprising a solid metallic glass. According to the method, a preform is shaped below the glass transition temperature and is then heated to a temperature above the glass transition temperature.
-
公开(公告)号:US20220118511A1
公开(公告)日:2022-04-21
申请号:US17427597
申请日:2020-01-30
Applicant: Heraeus Amloy Technologies GmbH
Inventor: Tim Gläser , Hamed Shakur Shahabi , Eugen Milke , Hans-Jürgen Wachter
Abstract: A method for production of an ingot of a bulk glass-forming alloy, comprising the steps of: Providing a homogeneous melt of a bulk glass-forming alloy; casting the homogeneous melt into a casting mould, whereby the casting mould does not cool down below the glass-transition temperature of the alloy at the contact surface to the melt for at least 5 seconds; and cooling down the melt below the glass transition temperature of the bulk glass-forming alloy while obtaining the ingot.
-
-