公开(公告)号:US6060579A
公开(公告)日:2000-05-09
申请号:US47556
申请日:1998-03-25
申请人: Hiroyuki Ohme , Motoki Hiratsuka , Katsuo Nogami
发明人: Hiroyuki Ohme , Motoki Hiratsuka , Katsuo Nogami
摘要: A method for producing polybutylene terephthalate comprising continuously esterifying a dicarboxylic acid component consisting essentially of terephthalic acid with a diol component consisting essentially of 1,4-butanediol followed by polycondensing the resulting oligomer, wherein the esterification is effected in a molar ratio, P, of the diol component to the dicarboxylic acid component to fall between 1.1 and 1.6, in the presence of a combination of an organic titanium compound and an organic tin compound that satisfies the following requirement:amount of organic titanium compound (mol %).ltoreq.0.08.times.P-0.07where P=molar ratio of diol component to dicarboxylic acid component, and is followed by the polycondensation.
摘要翻译: 一种聚对苯二甲酸丁二醇酯的制造方法,其特征在于,将基本上由对苯二甲酸组成的二羧酸成分与主要由1,4-丁二醇组成的二醇成分连续酯化,然后使得到的低聚物缩聚,其中酯化反应的摩尔比P 在有机钛化合物和有机锡化合物的组合的存在下,二羧酸成分降解至1.1〜1.6,有机钛化合物的含量满足以下要求:有机钛化合物的量(摩尔%)≤0.08 xP-0.07其中P =二醇组分与二羧酸组分的摩尔比,然后进行缩聚。