公开(公告)号:US3728106A
公开(公告)日:1973-04-17
申请号:US3728106D
申请日:1969-11-13
Applicant: INT NICKEL CO
Inventor: BADIA F , ANDERSON D , KIRBY G
IPC: C22C9/06
CPC classification number: C22C9/06
Abstract: WROUGHT COPPER-NICKEL ALLOYS CONTAINING SPECIAL AMOUNTS OF CHROMIUN EXHIBIT IMPROVED RESISTANCE TO THE IMPINGEMENT EROSION EFFECTS OF HIGH VELOCITY SEAWATER. SMALL AMOUNT OF IRON ALSO IMPROVE "PARTING" CORROSION CHARACTERISTICS OF ALLOYS OF LOWER NICKEL CONTENT.
-
公开(公告)号:US3776473A
公开(公告)日:1973-12-04
申请号:US3776473D
申请日:1972-03-27
Applicant: INT NICKEL CO
CPC classification number: B22F1/0055 , B22F9/04 , B22F2009/043 , B22F2998/00 , C01P2004/03 , C01P2004/20 , C01P2004/50 , C01P2004/61 , C01P2004/62 , C01P2006/60 , C09C1/646 , C22C1/0416
Abstract: Aluminum flake powder having high specular reflectivity is produced by wet ball milling aluminum powder in the presence of a lubricant using a volume ratio of grinding balls to powder of at least 15:1 and a volume ratio of grinding balls to milling liquid (e.g., a light liquid hydrocarbon) which preferably is substantially equal.
Abstract translation: 具有高镜面反射率的铝片粉末在润滑剂存在下通过湿式球磨铝粉生产,使用研磨球与粉末的体积比至少为15:1,研磨球与研磨液体的体积比(例如, 轻液烃),其优选基本相等。
-
公开(公告)号:US3753694A
公开(公告)日:1973-08-21
申请号:US3753694D
申请日:1970-07-06
Applicant: INT NICKEL CO
Inventor: BADIA F , MAC DONALD D , ANSUINI F
CPC classification number: B22D19/14 , B22F1/025 , C22C1/1036 , C22C49/14 , C22C2001/1047 , Y10T428/12486
Abstract: Composites formed of incompatible constituents, i.e., constituents which are mutually insoluble, are produced by introducing at least one such constituent in coated form into a molten bath of the other, the bath being subjected to the influence of a vortex.
Abstract translation: 通过将不相容的成分即相互不溶的组分形成的复合材料通过将至少一种这样的涂层形式的组分引入到另一种的熔融浴中而产生,浴受到涡流的影响。
-
-