摘要:
A vegetation enhancement composite including a vegetation enhancement agent consisting of a first member selected from the group consisting of at least one macronutrient, micronutrient, nitrogen fertilizer including an inhibitor of nitrification activity, slow release fertilizer, and mixtures of such members and a pesticide; and at least one first controlled release film including a sulfonated polymer coating at least a portion of a surface of the vegetation enhancement agent. A method of producing controlled release fertilizers involving providing a vegetation enhancement agent consisting of a first member selected from the group consisting of at least one macronutrient, micronutrient, nitrogen fertilizer including an inhibitor of urease, nitrogen fertilizer including an inhibitor of nitrification activity, slow release fertilizer, and mixtures of such members and a pesticide; and coating at least one surface of the vegetation enhancement agent with a sulfonated polymer dissolved in a solvent system including an organic liquid to form a controlled release coating on the vegetation enhancement agent. An agricultural process involving the application of a vegetable enhancement agent coated with a sulfonated polymer to plant growth medium to stimulate germination and enhance growth of vegetable matter.
摘要:
A composite comprising a substrate and an elastomeric coating adhered to at least one surface of said substrate, said elastomeric coating having a thickness of about 1 to about 100 micrometers, wherein said elastomeric coating comprises an interpolymeric complex of a neutralized sulfonated polymer and an amine containing polymer, said neutralized sulfonated polymer having a sulfonate content of about 4 to about 200 meq. per 100 grams of said neutralized sulfonated polymer and said amine containing polymer containing basic nitrogen atoms wherein the basic nitrogen content ranges from about 4 to about 500 meq. per 100 grams of polymer.
摘要:
A composite comprising a substrate and a polymeric coating adhered to at least one surface of said substrate, said polymer coating having a thickness of about 1 to about 100 micrometers, wherein said polymer coating comprises an ionically and covalently crosslinked neutralized carboxylated polymer having a carboxylate content of about 5 to about 300 meq. per 100 grams of said ionically and covalently crosslinked neutralized carboxylated polymer.
摘要:
A composite comprising a substrate and an elastomeric coating adhered to at least one surface of said substrate, said elastomeric coating having a thickness of about 1 to about 100 micrometers, wherein said elastomeric coating comprises a neutralized sulfonated polymer having a sulfonate content of about 4 to about 200 meq. per 100 grams of said neutralized sulfonated polymer.
摘要:
The present invention relates to a process for the encapsulation of a solid substrate with a neutralized sulfonated polymer, which comprises the steps of: (a) forming a solution of a non-conjugated, diene polymer in a solvent selected from the group consisting of aliphatic, aromatic hydrocarbons and mixtures thereof; (b) contacting the solution of the unsaturated polymer with a sulfonating agent at a sufficient temperature and for a sufficient period of time to form a solution of a sulfonated polymer containing free acid; (c) forming a solution of a base selected from the group consisting of alkali metal hydroxides and mixtures thereof in a mixtrue of an aliphatic alcohol and a hydrocarbon, the hydrocarbon being selected from the group consisting of aliphatic and aromatic hydrocarbons and mixtures thereof; (d) adding the solution of base to the solution of sulfonated polymer in an amount sufficient to neutralize the polymer and the free acid, thereby forming a coating solution; (e) contacting the solid substrate with the coating solution while removing the solvent therefrom, thereby forming an encapsulated substrate. In a preferred embodiment, the solvent removed during step (e) is recovered and distilled to separate the solvent into at least two fractions, a fraction containing substantially hydrocarbon and an alcohol containing fraction. The separated solvents are then recycled to dissolve the polymer in step (a) and to dissolve the base in step (c).
摘要:
An encapsulated water soluble fertilizer which comprises a polymeric film of about 2 to about 100 micrometers coated on a surface of said fertilizer, said polymeric film comprising a sulfonated polymer having about 10 to about 200 meq of sulfonate groups per 100 grams of said sulfonated polymer, said sulfonate groups being neutralized with a polycaprolactone polymer being characterized by the formula ##STR1## wherein R.sub.1 and R.sub.2 is an alkyl, cycloalkyl or aryl group; R.sub.3, R.sub.4 and R.sub.5 are a hydrogen or alkyl, cycloalkyl, or aryl groups; m equals 1 to 20 and n equals 1 to 500.
摘要:
A composite comprising a urea substrate and ionically and covalently crosslinked, neutralized, sulfonated EPDM elastomeric coating encapsulating the urea.
摘要:
An encapsulated breaker chemical composition used in an oil or gas stimulation operation which comprises: a breaker chemical; and a pinhole free coating of an ionically and covalently crosslinked neutralized sulfonated elastomeric polyer of about 2 to about 80 microns thick deposited onto the surface of the breaker chemical, wherein said polymer encapsulates the breaker chemical, wherein the polymer is permeable to the breaker chemical and the polymer is non-reactive to the breaker chemical.
摘要:
An encapsulated breaker chemical composition used in an oil or gas stimulation operation which comprises: a breaker chemical; and a pinhole free coating of an ionically and covalently crosslinked neutralized sulfonated elastomeric polymer of about 2 to about 80 microns thick deposited onto the surface of the breaker chemical, wherein said polymer encapsulates the breaker chemical, wherein the polymer is permeable to the breaker chemical and the polymer is non-reactive to the breaker chemical.
摘要:
A polymeric composite comprising a (a) urea; (b) a coating of sulfonated polymer which has about 10 to about 200 meq. of sulfonate groups per 100 grams of said sulfonated polymer, said sulfonate groups being neutralized with a polycaprolactone polymer having the formula: ##STR1## wherein R.sub.1 or R.sub.2 is an alkyl, cycloalkyl or aryl group; R.sub.3, R.sub.4 and R.sub.5 are a hydrogen or alkyl, cycloalkyl, or aryl groups; m equals 1 to 20 and n equals 1 to 500, wherein said coating is deposited on the surface of said urea.