Method for making high volume reinforced aluminum composite by use of dipping process
    1.
    发明授权
    Method for making high volume reinforced aluminum composite by use of dipping process 有权
    使用浸渍法制造高容量增强铝复合材料的方法

    公开(公告)号:US06406516B1

    公开(公告)日:2002-06-18

    申请号:US09846414

    申请日:2001-05-01

    IPC分类号: C22C100

    摘要: Disclosed are composition and a method for making a high volume reinforced Al composite by use of a dipping process. Through the method comprising mixing 20-50 wt % of exothermic reaction-causing Ti and C or Ti and B powders, 20-60 wt % of exothermic reaction-controlling diluent powders, and 5-30 wt % of infiltration-aiding Al or Al alloy powders, then preparing mixture powders; preforming the mixture powders into a predetermined shape; fitting the preformed body in a reaction container, followed by dipping in an Al melt of 700-1,100° C.; and separating the synthesized composite from the reaction container after removal from the Al melt, a high volume reinforced Al composite can be prepared from the mixture powders through such exothermic synthesis in a metal melt that reinforced particles are uniformly distributed while restraining the generation of pores. As such, the exothermic reaction-controlling diluent powders are selected from the group consisting of TiC, TiB2, SiC, WC or mixtures thereof.

    摘要翻译: 公开了通过浸渍方法制备高体积增强Al复合材料的组合物和方法。 通过包括混合20-50重量%的放热反应的Ti和C或Ti和B粉末,20-60重量%的放热反应控制稀释剂粉末和5-30重量%的渗透助剂Al或Al 合金粉末,然后制备混合粉末; 将混合物粉末预成形为预定形状; 将预成型体装配在反应容器中,随后浸入700-1100℃的Al熔体中; 并在从Al熔体中除去后将合成的复合物从反应容器中分离出来,可以通过在金属熔体中的这种放热合成从混合物粉末制备高体积的增强的Al复合材料,其中增强的颗粒均匀分布,同时抑制孔的产生。 因此,放热反应控制稀释剂粉末选自TiC,TiB2,SiC,WC或其混合物。