公开(公告)号:US07150922B2
公开(公告)日:2006-12-19
申请号:US10248056
申请日:2002-12-13
申请人: Irene Spitsberg , Joseph David Rigney , Ramgopal Darolia , Elissa Hae-Kyung Lee , Jeffrey Allan Pfaendtner
发明人: Irene Spitsberg , Joseph David Rigney , Ramgopal Darolia , Elissa Hae-Kyung Lee , Jeffrey Allan Pfaendtner
CPC分类号: C23C28/321 , C21D7/06 , C23C4/18 , C23C8/02 , C23C26/00 , C23C28/345 , C23C28/3455 , Y10T428/12611 , Y10T428/12736 , Y10T428/12937 , Y10T428/12944
摘要: A beta-phase nickel aluminide (NiAl) overlay coating (24) and method for modifying the grain structure of the coating (24) to improve its oxidation resistance. The coating (24) is deposited by a method that produces a grain structure characterized by grain boundaries (44) exposed at the outer coating surface (36). The grain boundaries (44) may also contain precipitates (40) as a result of the alloyed chemistry of the coating (24). During or after deposition, the overlay coating (24) is caused to form new grain boundaries (34) that, though open to the outer surface (36) of the coating (24), are free of precipitates or contain fewer precipitates (40) than the as-deposited grain boundaries (44). New grain boundaries (34) are preferably produced by causing the overlay coating (24) to recrystallize during coating deposition or after deposition as a result of a surface treatment followed by heat treatment.
摘要翻译: β相镍铝化合物(NiAl)覆盖层(24)以及用于改变涂层(24)的晶粒结构以提高其抗氧化性的方法。 通过产生以在外涂层表面(36)处暴露的晶界(44)为特征的晶粒结构的方法沉积涂层(24)。 由于涂层(24)的合金化学,晶界(44)也可含有沉淀物(40)。 在沉积期间或之后,使覆盖涂层(24)形成新的晶粒边界(34),其尽管向涂层(24)的外表面(36)开口,但没有沉淀物或含有较少的沉淀物(40) 比沉积的晶界(44)。 优选通过在涂布沉积期间或沉积后的覆盖涂层(24)进行再结晶,然后进行热处理后的表面处理,来制造新的晶界(34)。