公开(公告)号:US20180001377A1
公开(公告)日:2018-01-04
申请号:US15546401
申请日:2016-01-22
Applicant: JFE STEEL CORPORATION
Inventor: Keigo TOISHI , Hiroyuki OHNO , Norichika ARAMAKI , Yuji MIKI
IPC: B22D11/124 , B22D11/20
CPC classification number: B22D11/1246 , B21B1/466 , B21B2201/14 , B22D11/1206 , B22D11/1282 , B22D11/20 , B22D11/207 , B22D11/225
Abstract: Provided is a continuous casting method of steel that prevents a solidification completion position from being changed even when a drawing speed V of a cast slab is changed. The method includes drawing a cast slab by setting a drawing speed V0 while spraying cooling water to the cast slab at a cooling water spray amount W0 [kg/ton-cast slab]. Then, changing the drawing speed to the speed V1 while spraying cooling water to the cast slab at a cooling water spray amount W1 [kg/ton-cast slab]. The method further includes spraying cooling water to the cast slab at a cooling water spray amount Wt [kg/ton-cast slab] during a period of time t that is obtained by dividing a target length Lt by the drawing speed V0. The water spray amount Wt satisfying either formula (1): Wt W1 under a condition of V1>V0.