Thick film conductor employing nickel oxide
    1.
    发明授权
    Thick film conductor employing nickel oxide 失效
    使用氧化镍的厚膜导体

    公开(公告)号:US4317750A

    公开(公告)日:1982-03-02

    申请号:US180446

    申请日:1980-08-22

    摘要: A thick film conductor, a process for producing such, and a thick film conductor paste of:A. 12 to 25 weight percent boron; andB. zero to 35 weight percent glass frit; andC. balance essentially nickel oxide;wherein the combined weight of boron and glass frit is 22 to 45 percent by weight of the paste, all weight percentages being on a dry basis.