公开(公告)号:US11753694B1
公开(公告)日:2023-09-12
申请号:US18023395
申请日:2022-06-06
申请人: JIANGSU UNIVERSITY
发明人: Jianzhong Zhou , Yanqiang Gou , Li Li , Yu Zhang , Xiankai Meng , Shu Huang , Gaoqiang Jiang , Pengfei Li , Xv Feng
CPC分类号: C21D10/005 , C22C21/00
摘要: A pulse current-assisted laser peen forming and hydrophobic surface preparing method for an aluminum alloy includes the following steps: placing a pretreated aluminum alloy onto a shock platform, where electrodes are respectively provided at two ends of the aluminum alloy, and flowing silicone oil covers a surface of the aluminum alloy; determining a laser energy; applying a high-frequency pulse current to the surface of the aluminum alloy through the electrodes, where a shot peening laser generates a laser beam according to the laser energy to shock the surface of the aluminum alloy, and under an action of an electrical pulse and laser shock, the aluminum alloy shows a bent arc-shaped surface, with a shock surface forming a porous micro-nano multi-stage surface; and performing chemical modification on the shock surface of the aluminum alloy to reduce a surface energy of the material, thereby obtaining a super-hydrophobic arc-shaped aluminum alloy surface.
-
公开(公告)号:US12128501B2
公开(公告)日:2024-10-29
申请号:US18286758
申请日:2022-07-08
申请人: Jiangsu University
发明人: Jianzhong Zhou , Lei Huang , Yanqiang Gou , Xiankai Meng , Shu Huang , Pengfei Li , Li Li , Gaoqiang Jiang , Xu Feng
IPC分类号: B23K26/356 , C21D10/00 , C22C21/00 , C23C22/02 , C23C22/05 , B23K101/34 , B23K103/10
CPC分类号: B23K26/356 , C21D10/005 , C22C21/00 , C23C22/02 , C23C22/05 , B23K2101/35 , B23K2103/10 , C23C2222/20
摘要: The present disclosure provides a method for preparing a superhydrophobic surface of an aluminum alloy through laser peening, including the following steps: coating a surface of the aluminum alloy as an absorption layer with an organic component-containing confinement layer to obtain a coated aluminum alloy, where the organic component-containing confinement layer is a mixed organic solution including 5 mL to 10 mL of perfluorooctyltriethoxysilane (FOTS), 100 mL to 200 mL of absolute ethanol, and 30 mL to 50 mL of distilled water; and subjecting a surface of the coated aluminum alloy to the laser peening to form the superhydrophobic surface.
-