Functionalized amine initiators for anionic polymerization
    1.
    发明授权
    Functionalized amine initiators for anionic polymerization 失效
    用于阴离子聚合的官能化胺引发剂

    公开(公告)号:US5605872A

    公开(公告)日:1997-02-25

    申请号:US459585

    申请日:1995-06-02

    CPC分类号: C08F12/04 C08F36/04

    摘要: A process for the preparation of hydrocarbon solutions of monofunctional amine initiators of the following general structures: ##STR1## wherein M is defined as an alkali metal, selected from the group consisting of lithium, sodium and potassium, Q is a saturated or unsaturated hydrocarbyl group derived by incorporation of a compound selected from the group consisting of conjugated diene hydrocarbons and alkenyl substituted aromatic hydrocarbons; Z is a hydrocarbon tether group which contains 3-25 carbon atoms; A is an element selected from Group IVa of the periodic table and R.sup.1, R.sup.2, and R.sup.3 are independently selected from hydrogen, alkyl, substituted alkyl, cycloalkyl, aryl or substituted aryl groups, m is an integer from 0 to 7, and n is an integer from 1 to 5, monofunctional amine initiators produced by the process, use of the initiators in a polymerization process and polymers produced by the polymerization process.

    摘要翻译: 制备以下一般结构的单官能胺引发剂的烃溶液的方法:MQnZN(A(R1R2R3))2金属,选自锂,钠和钾,Q是衍生的饱和或不饱和烃基 通过并入选自共轭二烯烃和烯基取代的芳族烃的化合物; Z是含有3-25个碳原子的烃系链基团; A是选自元素周期表IVa的元素,R1,R2和R3独立地选自氢,烷基,取代的烷基,环烷基,芳基或取代的芳基,m是0-7的整数,n是 1至5的整数,通过该方法制备的单官能胺引发剂,在聚合方法中使用引发剂和通过聚合方法制备的聚合物。

    Functionalized amine initiators for anionic polymerization
    2.
    发明授权
    Functionalized amine initiators for anionic polymerization 失效
    用于阴离子聚合的官能化胺引发剂

    公开(公告)号:US5527753A

    公开(公告)日:1996-06-18

    申请号:US354998

    申请日:1994-12-13

    CPC分类号: C08F12/04 C08F36/04

    摘要: A process for the preparation of hydrocarbon solutions of monofunctional amine initiators of the following general structures: ##STR1## wherein M is defined as an alkali metal, selected from the group consisting of lithium, sodium and potassium, Q is a saturated or unsaturated hydrocarbyl group derived by incorporation of a compound selected from the group consisting of conjugated diene hydrocarbons and alkenyl substituted aromatic hydrocarbons; Z is a hydrocarbon tether group which contains 3-25 carbon atoms; A is an element selected from Group IVa of the periodic table and R.sup.1, R.sup.2, and R.sup.3 are independently selected from hydrogen, alkyl, substituted alkyl, cycloalkyl, aryl or substituted aryl groups, m is an integer from 0 to 7, and n is an integer from 1 to 5, monofunctional amine initiators produced by the process, use of the initiators in a polymerization process and polymers produced by the polymerization process.

    摘要翻译: 制备以下一般结构的单官能胺引发剂的烃溶液的方法:MQnZN(A(R1R2R3))2金属,选自锂,钠和钾,Q是衍生的饱和或不饱和烃基 通过并入选自共轭二烯烃和烯基取代的芳族烃的化合物; Z是含有3-25个碳原子的烃系链基团; A是选自元素周期表IVa的元素,R1,R2和R3独立地选自氢,烷基,取代的烷基,环烷基,芳基或取代的芳基,m是0-7的整数,n是 1至5的整数,通过该方法制备的单官能胺引发剂,在聚合方法中使用引发剂和通过聚合方法制备的聚合物。

    Functionalized amine initiators for anionic polymerization
    3.
    发明授权
    Functionalized amine initiators for anionic polymerization 失效
    用于阴离子聚合的官能化胺引发剂

    公开(公告)号:US5523364A

    公开(公告)日:1996-06-04

    申请号:US458198

    申请日:1995-06-02

    CPC分类号: C08F12/04 C08F36/04

    摘要: A process for the preparation of hydrocarbon solutions of monofunctional amine initiators of the following general structures: ##STR1## wherein M is defined as an alkali metal, selected from the group consisting of lithium, sodium and potassium, Q is a saturated or unsaturated hydrocarbyl group derived by incorporation of a compound selected from the group consisting of conjugated diene hydrocarbons and alkenyl substituted aromatic hydrocarbons; Z is a hydrocarbon tether group which contains 3-25 carbon atoms; A is an element selected from Group IVa of the periodic table and R.sup.1, R.sup.2, and R.sup.3 are independently selected from hydrogen, alkyl, substituted alkyl, cycloalkyl, aryl or substituted aryl groups, m is an integer from 0 to 7, and n is an integer from 1 to 5, monofunctional amine initiators produced by the process, use of the initiators in a polymerization process and polymers produced by the polymerization process.

    摘要翻译: 制备以下一般结构的单官能胺引发剂的烃溶液的方法:其中M定义为碱金属,其选自锂,钠和钾,Q是饱和或 通过引入选自共轭二烯烃和烯基取代的芳族烃的化合物衍生的不饱和烃基; Z是含有3-25个碳原子的烃系链基团; A是选自元素周期表IVa的元素,R1,R2和R3独立地选自氢,烷基,取代的烷基,环烷基,芳基或取代的芳基,m是0-7的整数,n是 1至5的整数,通过该方法制备的单官能胺引发剂,在聚合方法中使用引发剂和通过聚合方法制备的聚合物。

    Functionalized amine initiators for anionic polymerization
    4.
    发明授权
    Functionalized amine initiators for anionic polymerization 失效
    用于阴离子聚合的官能化胺引发剂

    公开(公告)号:US5550203A

    公开(公告)日:1996-08-27

    申请号:US460305

    申请日:1995-06-02

    CPC分类号: C08F12/04 C08F36/04

    摘要: A process for the preparation of hydrocarbon solutions of monofunctional amine initiators of the following general structures:M--Q.sub.n --Z--N(A(R.sup.1 R.sup.2 R.sup.3)).sub.2or ##STR1## wherein M is defined as an alkali metal, selected from the group consisting of lithium, sodium and potassium, Q is a saturated or unsaturated hydrocarbyl group derived by incorporation of a compound selected from the group consisting of conjugated diene hydrocarbons and alkenyl substituted aromatic hydrocarbons; Z is a hydrocarbon tether group which contains 3-25 carbon atoms; A is an element selected from Group IVa of the periodic table and R.sup.1, R.sup.2, and R.sup.3 are independently selected from hydrogen, substituted alkyl, cycloalkyl, aryl or substituted aryl groups, m is an integer from 0 to 7, and n is an integer from 1 to 5, monofunctional amine initiators produced by the process, use of the initiators in a polymerization process and polymers produced by the polymerization process.

    摘要翻译: 制备以下一般结构的单官能胺引发剂的烃溶液的方法:选自锂,钠和钾的M-Qn-ZN(A(R1R2R3))2金属,Q是饱和或 通过引入选自共轭二烯烃和烯基取代的芳族烃的化合物衍生的不饱和烃基; Z是含有3-25个碳原子的烃系链基团; A是选自元素周期表Ⅳa的元素,R 1,R 2和R 3独立地选自氢,取代的烷基,环烷基,芳基或取代的芳基,m是0至7的整数,n是整数 1至5个,通过该方法制备的单官能胺引发剂,在聚合过程中使用引发剂和通过聚合方法制备的聚合物。

    Catalyzed hydrocarbyllithium process
    8.
    发明授权
    Catalyzed hydrocarbyllithium process 失效
    催化烃基锂工艺

    公开(公告)号:US5340507A

    公开(公告)日:1994-08-23

    申请号:US035998

    申请日:1993-03-23

    摘要: A catalytic process for alkylating an alkali metal selected from lithium, sodium and potassium with an alkyl halide containing 3 to 20 carbon atoms comprising conducting the reaction in the presence of a catalytic compound represented by the formula(RR.sup.1 R.sup.2 M.sup.a).sub.y A(R.sup.3).sub.xwherein R, R.sup.1 and R.sup.2 are independently selected from hydrogen, halogen, alkyl, alkenyl, cycloalkyl, and aryl groups, R.sup.3 is independently selected from alkyl groups containing 1 to 10 carbon atoms, alkylene groups containing 2 to 5 carbon atoms, aryl groups containing 6 to 18 carbon atoms, four to six-membered heterocyclic carbon containing groups containing one to two hetero atoms selected from oxygen, nitrogen, and sulfur; hydroxyalkyl, alkoxyalkyl and monoalkylaminoalkyl and dialkylaminoalkyl groups containing 2 to 13 carbon atoms; M.sup.a is selected from silicon, carbon, germanium, and tin, A is selected from oxygen, sulfur, nitrogen and phosphorus, and x and y independently have values from zero to three.

    摘要翻译: 一种用含有3-20个碳原子的烷基卤烷基化选自锂,钠和钾的碱金属的催化方法,包括在由式(RR1R2Ma)yA(R3)x表示的催化化合物存在下进行反应,其中R R 1和R 2独立地选自氢,卤素,烷基,烯基,环烷基和芳基,R 3独立地选自含有1至10个碳原子的烷基,含2至5个碳原子的亚烷基,含6至 18个碳原子,含有1至2个选自氧,氮和硫的杂原子的含有4至6元杂环碳的基团; 羟基烷基,烷氧基烷基和单烷基氨基烷基和含有2至13个碳原子的二烷基氨基烷基; Ma选自硅,碳,锗和锡,A选自氧,硫,氮和磷,x和y独立地具有从零到三的值。

    Preparation of lithium alkoxides
    9.
    发明授权
    Preparation of lithium alkoxides 失效
    锂盐的制备

    公开(公告)号:US5276219A

    公开(公告)日:1994-01-04

    申请号:US973116

    申请日:1992-11-06

    IPC分类号: C07C29/70 C07C31/30 C07F1/02

    CPC分类号: C07C29/70

    摘要: A process for producing clear, colorless solutions of branched lithium alkoxides containing 3 to 12 carbon atoms, in a polar reaction solvent, comprising reacting a dispersion of lithium metal having a particle size less than 300 microns with a minimum of 5 mole percent excess over stoichiometric of a branched alkyl alcohol containing 4 to 12 carbon atoms, in a polar reaction solvent as the reaction medium, at a temperature between 50.degree. C. and the boiling point of the solvent in an inert atmosphere.

    摘要翻译: 一种在极性反应溶剂中生产含有3至12个碳原子的支链烷氧基化物的透明无色溶液的方法,包括将粒度小于300微米的锂金属分散体与超过化学计量比的至少5摩尔%过量反应 的在极性反应溶剂中作为反应介质的含有4至12个碳原子的支链烷基醇在惰性气氛中在50摄氏度和溶剂的沸点之间。

    Organoalkali compounds and their preparation
    10.
    发明授权
    Organoalkali compounds and their preparation 失效
    有机碱化合物及其制备方法

    公开(公告)号:US5976403A

    公开(公告)日:1999-11-02

    申请号:US65782

    申请日:1998-04-23

    摘要: A process for producing dispersions of atmospherically stable, coated alkali metal particles and atmospherically stable, coated alkali metal powders by agitating a mixture of molten alkali metal in a hydrocarbon oil at dispersion speeds, optionally in the presence of a dispersing agent, contacting the molten alkali metal-hydrocarbon oil dispersion, above or below the surface of the dispersion, with up to 3 weight percent anhydrous carbon dioxide while agitating the dispersion for at least 1 minute. The dispersion in oil can be used directly in chemical reactions. The bulk of the oil can be removed from the dispersions to produce oil wet particles, the oil wet particles car be washed with a low boiling hydrocarbon to produce hydrocarbon wet particles which can be dried to produce atmospherically stable powders of coated metal particles. The dispersed particles in oil, the oil wet particles, the hydrocarbon wet particles and the atmospherically stable powders can each be used in chemical reactions. After washing and drying, the process produces lithium powders having a surface coating composition containing 0.1-0.3 atom percent lithium, 0.3-0.4 atom percent carbon, and 0.3-0.5 atom percent oxygen. The products of the invention may be used to synthesize organometallic compounds, esp. n-butyl lithium and sec-butyl lithium, having low color and low soluble inorganic chloride levels.

    摘要翻译: 通过搅拌熔融碱金属在烃油中的分散速度的混合物,任选地在分散剂存在下,使熔融碱接触,制备大气稳定的涂覆的碱金属颗粒和大气稳定的包覆的碱金属粉末的分散体的方法 在分散体表面上方或下方的金属 - 烃油分散体与最多3重量%的无水二氧化碳同时搅拌分散体至少1分钟。 油中的分散体可以直接用于化学反应。 大部分油可以从分散体中除去以产生油湿颗粒,用低沸点烃洗涤油湿颗粒汽车以产生烃湿颗粒,其可以被干燥以产生大气稳定的涂覆金属颗粒的粉末。 油中的分散颗粒,油湿颗粒,烃湿颗粒和气氛稳定的粉末均可用于化学反应。 洗涤和干燥后,该方法产生具有表面涂层组合物的锂粉末,其中含有0.1-0.3%原子百分比的锂,0.3-0.4%的碳和0.3-0.5%的氧。 本发明的产品可用于合成有机金属化合物, 正丁基锂和仲丁基锂,颜色低,可溶性无机氯化物水平低。