Method for the production of potassium chloride with K.sub.2 O content
of more than 55 weight percent
    2.
    发明授权
    Method for the production of potassium chloride with K.sub.2 O content of more than 55 weight percent 失效
    用K2O含量超过55重量百分比生产氯化钾的方法

    公开(公告)号:US5057208A

    公开(公告)日:1991-10-15

    申请号:US256062

    申请日:1988-10-06

    IPC分类号: B03D1/01 B03D1/02 C01D3/08

    摘要: In a method for manufacturing potassium chloride with a K.sub.2 O content of 55 wt. % from the fine salt resulting from the decomposition of carnallite, n-alkyl amine salts are used as conditioning agents, and flotation media containing magnesium and potassium chloride are used to separate this fine decomposition salt in an initial flotation stage into a grain size fraction of 0.315. After the conditioning, this residue is again floated and the potassium chloride comes to the surface as a second pre-concentrate. Then the potassium chloride is separated from the mixture of the two pre-concentrates, without any further conditioning, in another flotation stage, and collected.

    摘要翻译: 在K2O含量为55重量%的氯化钾的制造方法中, 来自由光卤石分解产生的细盐的%,使用正烷基胺盐作为调理剂,并且使用含有镁和氯化钾的浮选介质将初始浮选阶段中的这种细分解盐分离成粒度分数 作为第一预浓缩物<0.1mm,粒径> 0.315的残渣。 调理后,再次漂浮残余物,氯化钾作为第二预浓缩物进入表面。 然后在另一个浮选阶段将氯化钾与两种预浓缩物的混合物分离,无需任何进一步的调理,并收集。

    Process and apparatus for the electrostatic dressing of
carnallite-containing crude potassium salts
    3.
    发明授权
    Process and apparatus for the electrostatic dressing of carnallite-containing crude potassium salts 失效
    含光卤石的粗钾盐的静电敷料的方法和装置

    公开(公告)号:US4297207A

    公开(公告)日:1981-10-27

    申请号:US25521

    申请日:1979-03-30

    IPC分类号: B03C7/02 B03C7/12 B03B1/00

    CPC分类号: B03C7/12

    摘要: A carnallite-containing crude salt is separated into a carnallite fraction, a sylvite fraction and an abandonable residue by grinding the salt to an average particle size of about 1.5 mm., conditioning the particles in a conventional manner with from 5-300 g/t of a conventional conditioning agent adjusting the relative humidity of the conditioned particles to 5-25%, and subjecting the resulting particles to electrostatic separation in two stages, wherein in the first stage the particles are subjected to a high voltage electric field having a field length of 0.4 to 1.2 m to separate a carnallite fraction by imparting to the carnallite fraction a high sidewards velocity relative to the initial downward velocity upon entering the field, thereby causing deflection of the carnallite away from a middlings fraction, and wherein in the second stage the first stage middling fracton is subjected to a second high voltage electric field having a field length of 1.5 to 2.5 m to f or m a sylvite fraction, a second middlings fraction which also has a high sidewards velocity imparted thereto relative to the initial downward velocity upon entry into the second field thereby causing deflection of the sylvite fraction away from and an abandonable residue which has a sidewards velocity imparted thereto opposite in direction to the sidewards velocity of the sylvite for deflection therefrom and from the second middlings fraction.

    摘要翻译: 含有光卤石的粗盐通过将盐研磨至约1.5mm的平均粒径,分离成光卤石级分,硅藻土级分和可弃残余物,以常规方式用5-300g / t调理颗粒 将调节颗粒的相对湿度调节至5-25%的常规调理剂,并将所得颗粒进行两个阶段的静电分离,其中在第一阶段中,对颗粒进行具有场长度的高压电场 为0.4〜1.2μm,通过使光卤石部分在进入场时相对于初始向下速度施加高的侧向速度来分离光卤石部分,从而引起光卤石偏离中间部分,并且其中在第二阶段中 将第一阶段中间分枝经历场长为1.5至2.5μm的第二高电压电场至f或ma sylvite fra 第二中间部分在进入第二场时相对于初始向下速度赋予其较高的侧向速度,从而导致锯齿岩部分偏离,并且可抛弃的残余物具有向其相反的方向施加的侧向速度 以及从第二中间部分偏转的硅藻土的侧向速度。

    Process for the electrostatic separation of crude potash salts
    5.
    发明授权
    Process for the electrostatic separation of crude potash salts 失效
    粗制钾盐的静电分离方法

    公开(公告)号:US4276154A

    公开(公告)日:1981-06-30

    申请号:US21278

    申请日:1979-03-16

    CPC分类号: C01D3/08 B03C7/003

    摘要: Crude potash salt is conditioned for separation into its components by means of an electrostatic field by grinding the salt to disintegration and contacting the ground salt with a conditioning agent, such as salicylic acid, which has been converted to the gaseous state, such that the conditioning agent draws up onto the surfaces of the salt crystals by absorption. The quantity of the conditioning agent employed is adjusted by varying the evaporation temperature and/or by varying the volume of heated air and/or inert gas, serving as a carrier material.

    摘要翻译: 通过研磨盐将磨碎的盐与已经转化为气态的调节剂(如水杨酸)接触,使粗制的钾盐通过静电场分离成其组分,使得调理剂 药剂通过吸收吸附在盐晶体的表面上。 通过改变蒸发温度和/或通过改变用作载体材料的加热空气和/或惰性气体的体积来调节所用调理剂的量。

    Process for electrostatic separation of pyrite from crude coal
    6.
    发明授权
    Process for electrostatic separation of pyrite from crude coal 失效
    从原煤静电分离黄铁矿的方法

    公开(公告)号:US3941685A

    公开(公告)日:1976-03-02

    申请号:US497636

    申请日:1974-08-15

    IPC分类号: B03C7/00 B03B1/04

    CPC分类号: B03C7/003

    摘要: An improved process is disclosed for electrostatic separation of pyrite from powdered crude coal comprising vigorously mixing the powdered crude coal with a selected fatty acid glyceride as a conditioning substance and conducting the electrostatic separation at a relative humidity of 2.5-20% and a temperature between room temperature and 100.degree. C. In a multiple stage process yields of purified coal substantially greater than those of prior art processes can be obtained.

    摘要翻译: 公开了一种改进的方法,用于从粉末状粗煤中静电分离黄铁矿,其包括将粉末状粗煤与选择的脂肪酸甘油酯剧烈混合作为调理物质,并在2.5-20%的相对湿度和室温之间进行静电分离 温度和100℃。在多级方法中,可以获得比现有技术方法大得多的纯化煤的产率。