公开(公告)号:US09861796B2
公开(公告)日:2018-01-09
申请号:US14367091
申请日:2012-12-14
Applicant: KANEKA CORPORATION
Inventor: Shintaro Osumi , Yoichi Yamaguchi
CPC classification number: A61M25/1029 , A61M2025/1084 , B29C49/04 , B29C49/08 , B29C2071/022 , B29K2077/00 , B29K2105/258 , B29K2995/0053 , B29L2031/7543
Abstract: The present invention is a production method for an expansion balloon (2) for use in a balloon catheter (1), including the steps of; forming a balloon tube (8) by extrusion molding so as to have a cross section orthogonal to an axial direction with the shape of a circle on the outside and the shape of a polygon having a circumcircle on the inside; and placing the balloon tube (8) in a mold to perform biaxially-stretched blow molding to obtain the balloon, whereby it is possible to produce the expansion balloon (2) that has no unevenness in film thickness of a straight pipe part (4) and allows stable folding control by simple processes with favorable molding yields.
-
公开(公告)号:US20150021834A1
公开(公告)日:2015-01-22
申请号:US14367091
申请日:2012-12-14
Applicant: KANEKA CORPORATION
Inventor: Shintaro Osumi , Yoichi Yamaguchi
CPC classification number: A61M25/1029 , A61M2025/1084 , B29C49/04 , B29C49/08 , B29C2071/022 , B29K2077/00 , B29K2105/258 , B29K2995/0053 , B29L2031/7543
Abstract: The present invention is a production method for an expansion balloon (2) for use in a balloon catheter (1), including the steps of; forming a balloon tube (8) by extrusion molding so as to have a cross section orthogonal to an axial direction with the shape of a circle on the outside and the shape of a polygon having a circumcircle on the inside; and placing the balloon tube (8) in a mold to perform biaxially-stretched blow molding to obtain the balloon, whereby it is possible to produce the expansion balloon (2) that has no unevenness in film thickness of a straight pipe part (4) and allows stable folding control by simple processes with favorable molding yields.
Abstract translation: 本发明是一种用于球囊导管(1)的膨胀气囊(2)的制造方法,包括以下步骤: 通过挤出成型形成气囊管(8),以使得具有与轴向方向正交的横截面与外侧的圆形,以及在内侧具有外接圆的多边形的形状; 并将气囊管(8)放置在模具中进行双轴拉伸吹塑成型,得到球囊,由此能够制造直管部(4)的膜厚不均匀的膨胀气球(2) 并且通过简单的工艺允许稳定的折叠控制,并具有良好的成型产量。
-