公开(公告)号:US11472715B2
公开(公告)日:2022-10-18
申请号:US17169438
申请日:2021-02-06
摘要: The method of making carbon-zinc oxide (C—ZnO) nanoparticles includes grinding a mixture of zinc nitrate hexahydrate (Zn(NO3)2.6H2O) and furfural (C4H3OCHO) to produce a ground mixture. As a non-limiting example, the zinc nitrate hexahydrate (Zn(NO3)2.6H2O) and the furfural (C4H3OCHO) may be placed in a mortar and ground, by hand with a pestle, for approximately 10 minutes. The ground mixture is then heated to produce the C—ZnO nanoparticles. As a non-limiting example, the ground mixture may be heated in a quartz tube at a temperature of approximately 500° C.