Method of smelting copper
    1.
    发明授权
    Method of smelting copper 有权
    冶炼铜的方法

    公开(公告)号:US07955409B2

    公开(公告)日:2011-06-07

    申请号:US12502780

    申请日:2009-07-14

    IPC分类号: C22B7/04 C22B15/00

    摘要: A method of smelting copper includes: a generating step of generating blister and slag from copper matte by charging the copper matte into a smelting furnace and oxidizing the copper matte; a first refining step of refining another blister from the slag by reduction in an electrical furnace; and a charging step of charging the slag into one of the smelting furnace or another smelting furnace for treating copper concentrate and generating matte as repeating flux if copper grade of slag generated in the first refining step is higher than 0.8 weight %.

    摘要翻译: 一种熔炼铜的方法包括:通过将铜锍装入冶炼炉中并氧化铜锍而产生铜锍产生气泡和炉渣的产生步骤; 第一精炼步骤,通过在电炉中的还原从炉渣中除去另一个气泡; 以及在第一精炼步骤中产生的铜等级的渣高于0.8重量%的情况下,将炉渣装入冶炼炉或另一熔炼炉中的处理铜精矿并产生锍作为重复焊剂的充电步骤。

    Method of smelting copper
    2.
    发明授权
    Method of smelting copper 有权
    冶炼铜的方法

    公开(公告)号:US07918917B2

    公开(公告)日:2011-04-05

    申请号:US12502710

    申请日:2009-07-14

    IPC分类号: C22B15/06 C22B15/14

    摘要: A method of smelting copper includes: a generating step of generating blister and calcium ferrite slag from copper matte by charging the copper matte into a smelting furnace and oxidizing the copper matte; and a refining step of refining another blister from the calcium ferrite slag in an electrical furnace under a temperature condition of 1250 degrees C. to 1350 degrees C. and under a reductive atmosphere condition of oxygen partial pressure logPO2≦−9.3.

    摘要翻译: 一种熔炼铜的方法包括:通过将铜锍装入冶炼炉中并氧化铜锍,从铜锍产生水泡和铁酸钙矿渣的产生步骤; 在1250摄氏度至1350摄氏度的温度条件下,并在氧分压logPO2< l3; -9.3的还原性气氛条件下,在电炉中从钙铁氧体矿渣​​中精炼另一个气泡的精炼步骤。