Ozonation of carbon nanotubes in fluorocarbons
    1.
    发明申请
    Ozonation of carbon nanotubes in fluorocarbons 有权
    碳纳米管在碳氟化合物中的臭氧化

    公开(公告)号:US20060159612A1

    公开(公告)日:2006-07-20

    申请号:US11285232

    申请日:2005-11-22

    IPC分类号: C01B31/02 D01F9/127

    摘要: The present invention is generally directed to methods of ozonating CNTs in fluorinated solvents (fluoro-solvents), wherein such methods provide a less dangerous alternative to existing ozonolysis methods. In some embodiments, such methods comprise the steps of: (a) dispersing carbon nanotubes in a fluoro-solvent to form a dispersion; and (b) reacting ozone with the carbon nanotubes in the dispersion to functionalize the sidewalls of the carbon nanotubes and yield functionalized carbon nanotubes with oxygen-containing functional moieties. In some such embodiments, the fluoro-solvent is a fluorocarbon solvent, such as a perfluorinated polyether.

    摘要翻译: 本发明一般涉及在氟化溶剂(氟溶剂)中臭氧化碳纳米管的方法,其中这些方法对现有的臭氧分解方法提供了较不危险的替代方法。 在一些实施方案中,这些方法包括以下步骤:(a)将碳纳米管分散在氟溶剂中以形成分散体; 和(b)使臭氧与分散体中的碳纳米管反应,使碳纳米管的侧壁官能化,并产生具有含氧官能团的官能化碳纳米管。 在一些这样的实施方案中,氟 - 溶剂是氟烃溶剂,例如全氟化聚醚。

    Fibers comprised of epitaxially grown single-wall carbon nanotubes, and a method for added catalyst and continuous growth at the tip
    4.
    发明申请
    Fibers comprised of epitaxially grown single-wall carbon nanotubes, and a method for added catalyst and continuous growth at the tip 失效
    由外延生长的单壁碳纳米管组成的纤维,以及在尖端处添加催化剂和连续生长的方法

    公开(公告)号:US20070009421A1

    公开(公告)日:2007-01-11

    申请号:US11291449

    申请日:2005-12-01

    IPC分类号: D01F9/12

    摘要: The present invention is directed to fibers of epitaxially grown single-wall carbon nanotubes (SWNTs) and methods of making same. Such methods generally comprise the steps of: (a) providing a spun SWNT fiber; (b) cutting the fiber substantially perpendicular to the fiber axis to yield a cut fiber; (c) etching the cut fiber at its end with a plasma to yield an etched cut fiber; (d) depositing metal catalyst on the etched cut fiber end to form a continuous SWNT fiber precursor; and (e) introducing feedstock gases under SWNT growth conditions to grow the continuous SWNT fiber precursor into a continuous SWNT fiber.

    摘要翻译: 本发明涉及外延生长的单壁碳纳米管(SWNT)的纤维及其制造方法。 这样的方法通常包括以下步骤:(a)提供纺丝的SWNT纤维; (b)切割基本垂直于纤维轴线的纤维以产生切割的纤维; (c)用等离子体在其端部蚀刻切割的纤维,得到蚀刻的切割纤维; (d)将金属催化剂沉积在蚀刻的切割的纤维端上以形成连续的SWNT纤维前体; 和(e)在SWNT生长条件下引入原料气体以将连续的SWNT纤维前体生长成连续的SWNT纤维。