公开(公告)号:US5164015A
公开(公告)日:1992-11-17
申请号:US669032
申请日:1991-03-14
申请人: Klaus Kuhnke , Alexander Langner , Klaus Pflugbeil , Kurt Schindler , Dorothea Moldenhauer , Siegfried Kohler
发明人: Klaus Kuhnke , Alexander Langner , Klaus Pflugbeil , Kurt Schindler , Dorothea Moldenhauer , Siegfried Kohler
摘要: A method for cleaning a vessel by dissolving iron oxide present in the vessel includes introducing a saline solution into the vessel, the saline solution being formed of an acid acting as a complexing agent, of an alkalizing agent and of a reducing agent, the saline solution acting as an alkaline reducer; retaining the saline solution in the vessel for a given period of time at a temperature above 140.degree. C. and below the decomposition temperature of the anionic part of the saline solution for forming an iron complex; and subsequently removing the dissolved iron complex by emptying the vessel.
摘要翻译: 通过溶解存在于容器中的氧化铁来清洗容器的方法包括将盐溶液引入容器中,盐溶液由作为络合剂的酸,碱化剂和还原剂形成,盐水溶液 作为碱性还原剂; 将盐溶液在温度高于140℃并低于盐溶液的阴离子部分的分解温度下在容器中保持给定时间以形成铁络合物; 并随后通过排空容器去除溶解的铁络合物。
-
公开(公告)号:US5264041A
公开(公告)日:1993-11-23
申请号:US891686
申请日:1992-06-01
申请人: Klaus Kuhnke , Alexander Langner , Klaus Pflugbeil , Kurt Schindler , Dorothea Moldenhauer , Siegfried Kohler
发明人: Klaus Kuhnke , Alexander Langner , Klaus Pflugbeil , Kurt Schindler , Dorothea Moldenhauer , Siegfried Kohler
摘要: A method for cleaning a vessel by dissolving iron oxide present in the vessel includes introducing a saline solution into the vessel, the saline solution being formed of an acid acting as a complexing agent, of an alkalizing agent and of a reducing agent, the saline solution acting as an alkaline reducer; retaining the saline solution in the vessel for a given period of time at a temperature above 140.degree. C. and below the decomposition temperature of the anionic part of the saline solution for forming an iron complex; and subsequently removing the dissolved iron complex by emptying the vessel.
摘要翻译: 通过溶解存在于容器中的氧化铁来清洗容器的方法包括将盐溶液引入容器中,盐溶液由作为络合剂的酸,碱化剂和还原剂形成,盐水溶液 作为碱性还原剂; 将盐溶液在温度高于140℃并低于盐溶液的阴离子部分的分解温度下在容器中保持给定时间以形成铁络合物; 并随后通过排空容器去除溶解的铁络合物。
-
3.
公开(公告)号:US06841194B1
公开(公告)日:2005-01-11
申请号:US10732676
申请日:2003-12-10
CPC分类号: H01M2/0275 , H01M2/0217 , H01M2/0287 , H01M2/0292
摘要: A process for applying a graphite coating to the interior of a prismatic battery can by filling the can with a slurry containing graphite particles, immediately removing the slurry with an aspirating nozzle and then drying the residue left in the battery can to leave a thin film of graphite on the interior of the can. In a continuous process, fill nozzles and aspirating nozzles are moved in set into and out of the cans simultaneously, while moving the nozzles along with the cans through a fill and aspirate station on a conveyor. From there the cans travel through a drying oven where the residue remaining in the cans is dried to leave a thin uniform graphite film inside a prismatic can.
摘要翻译: 通过用含有石墨颗粒的浆料填充罐子,用吸液喷嘴立即除去浆料,然后干燥残留在电池罐中的残余物,从而将石墨涂层施加到棱柱形电池内部的方法可以留下薄膜 石墨在罐子的内部。 在连续过程中,将喷嘴和抽吸喷嘴同时移入和移出罐头,同时使喷嘴与罐一起移动通过输送机上的填充和抽吸站。 从那里,罐子通过干燥炉,其中残留在罐中的残余物被干燥以在棱柱形罐内留下薄的均匀的石墨膜。
-
-