公开(公告)号:US20160047057A1
公开(公告)日:2016-02-18
申请号:US14377503
申请日:2013-02-11
Applicant: MECAPROTEC INDUSTRIES
Inventor: PIERRE BARES , CELINE GAZEAU , CEDRIC STEPHAN , DAVID PEDELMAS , CLAUDE ROSSIGNOL , SYLVAIN BRUET , OLIVIER BRUCELLE , PAUL DEDIEU , PHILIPPE COMBES , LAURENT ARURAULT , VIVIANE TURQ , JEAN-JACQUES ROUSSE , KEVIN KLEPMAN
CPC classification number: C25D11/024 , C25D11/08 , C25D11/16 , C25D11/246 , C25D11/38
Abstract: A method for anodizing a part made of aluminum or an aluminum alloy by immersing the part in an aqueous bath essentially comprising sulfuric acid at a concentration of 150 to 250 g/L and at a temperature of 5 to 25° C. A DC voltage according to a voltage profile comprising a voltage increased at a rate of 1 to 32 V/min is applied to the part. The voltage is maintained at a plateau voltage value of 12 to 20 V for a duration sufficient for obtaining, at the surface of the part, an anode layer having a thickness of 3 to 7 μm and/or a layer weight of 20 to 150 mg/dm2.
Abstract translation: 将部分浸渍在基本上含有浓度为150〜250g / L的硫酸和5〜25℃的硫酸的水浴中,阳极氧化由铝或铝合金制成的部件的方法。 到包括以1至32V / min的速率增加的电压的电压分布被施加到该部分。 电压保持在12至20V的平台电压值,持续时间足以在部件的表面获得具有3至7μm厚度和/或层厚度为20至150mg的阳极层 / dm2。