摘要: The present invention relates to a catalyst, in particular for the preparation of phthalic anhydride by gas phase oxidation of o-xylene and/or naphthalene, having an inert support and at least one layer which has been applied thereto and has a catalytically active composition comprising TiO2, characterized in that at least a portion of the TiO2 used has the following properties: (a) the BET surface area is more than 15 m2/g, (b) at least 25% of the total pore volume is formed by pores having a radius between 60 and 400 nm, and (c) the primary crystal size is more than 22 ångstrøm. Also described is a preferred process for preparing such a catalyst, and the preferred use of the titanium dioxide used in accordance with the invention.
摘要翻译: 本发明涉及一种催化剂,特别是用于通过邻二甲苯和/或萘的气相氧化制备邻苯二甲酸酐,其具有惰性载体和至少一层已被施加到其上并具有催化活性组合物,该组合物包含 TiO 2 2,其特征在于所用的TiO 2的至少一部分具有以下性质:(a)BET表面积大于15μm2 (b)总孔体积的至少25%由半径在60和400nm之间的孔形成,(c)主晶体尺寸大于22μm。 还描述了制备这种催化剂的优选方法,以及根据本发明使用的二氧化钛的优选用途。
-
公开(公告)号:US07618918B2
公开(公告)日:2009-11-17
申请号:US11575789
申请日:2005-11-28
IPC分类号: B01J23/32 , C07D307/89
CPC分类号: B01J21/063 , B01J23/002 , B01J23/22 , B01J27/198 , B01J35/0006 , B01J35/0026 , B01J35/023 , B01J35/10 , B01J35/1014 , B01J35/1066 , B01J35/108 , B01J37/0219 , B01J37/0221 , B01J2523/00 , B01J2523/15 , B01J2523/47 , B01J2523/51 , B01J2523/53 , B01J2523/55
摘要: The present invention relates to a catalyst, in particular for the preparation of phthalic anhydride by gas phase oxidation of o-xylene and/or naphthalene, having an inert support and at least one layer which has been applied thereto and has a catalytically active composition comprising TiO2, characterized in that at least a portion of the TiO2 used has the following properties: (a) the BET surface area is more than 15 m2/g, (b) the primary crystal size is more than 210 ångstrøm. Also described is a preferred process for preparing such a catalyst, and the preferred use of the titanium dioxide used in accordance with the invention.
摘要翻译: 本发明涉及一种催化剂,特别是用于通过邻二甲苯和/或萘的气相氧化制备邻苯二甲酸酐,其具有惰性载体和至少一层已被施加到其上并具有催化活性组合物,该组合物包含 TiO 2,其特征在于所用的TiO 2的至少一部分具有以下性质:(a)BET表面积大于15m 2 / g,(b)初晶结晶尺寸大于210μm。 还描述了制备这种催化剂的优选方法,以及根据本发明使用的二氧化钛的优选用途。
-
公开(公告)号:US20080015364A1
公开(公告)日:2008-01-17
申请号:US11575789
申请日:2005-11-28
IPC分类号: B01J21/06 , B01J23/04 , C07D307/89
CPC分类号: B01J21/063 , B01J23/002 , B01J23/22 , B01J27/198 , B01J35/0006 , B01J35/0026 , B01J35/023 , B01J35/10 , B01J35/1014 , B01J35/1066 , B01J35/108 , B01J37/0219 , B01J37/0221 , B01J2523/00 , B01J2523/15 , B01J2523/47 , B01J2523/51 , B01J2523/53 , B01J2523/55
摘要: The present invention relates to a catalyst, in particular for the preparation of phthalic anhydride by gas phase oxidation of o-xylene and/or naphthalene, having an inert support and at least one layer which has been applied thereto and has a catalytically active composition comprising TiO2, characterized in that at least a portion of the TiO2 used has the following properties: (a) the BET surface area is more than 15 m2/g, (b) the primary crystal size is more than 210 ångstrøm. Also described is a preferred process for preparing such a catalyst, and the preferred use of the titanium dioxide used in accordance with the invention.
摘要翻译: 本发明涉及一种催化剂,特别是用于通过邻二甲苯和/或萘的气相氧化制备邻苯二甲酸酐,其具有惰性载体和至少一层已被施加到其上并具有催化活性组合物,该组合物包含 TiO 2 2,其特征在于所用的TiO 2的至少一部分具有以下性质:(a)BET表面积大于15μm2 SUP> / g,(b)初级晶体尺寸超过210østrstrøm。 还描述了制备这种催化剂的优选方法,以及根据本发明使用的二氧化钛的优选用途。
-
公开(公告)号:US08097558B2
公开(公告)日:2012-01-17
申请号:US11597495
申请日:2005-05-22
IPC分类号: C07D307/89 , B01J23/00
CPC分类号: B01J21/063 , B01J23/002 , B01J23/22 , B01J27/198 , B01J35/0006 , B01J35/0026 , B01J35/023 , B01J35/10 , B01J35/1014 , B01J35/1066 , B01J35/108 , B01J37/0219 , B01J37/0221 , B01J2523/00 , B01J2523/15 , B01J2523/47 , B01J2523/51 , B01J2523/53 , B01J2523/55
摘要: The present invention relates to a catalyst, in particular for the preparation of phthalic anhydride by gas phase oxidation of o-xylene and/or naphthalene, having an inert support and at least one layer which has been applied thereto and has a catalytically active composition comprising TiO2, characterized in that at least a portion of the TiO2 used has the following properties: (a) the BET surface area is more than 15 m2/g, (b) at least 25% of the total pore volume is formed by pores having a radius between 60 and 400 nm, and (c) the primary crystal size is more than 22 ångstrøm. Also described is a preferred process for preparing such a catalyst, and the preferred use of the titanium dioxide used in accordance with the invention.
摘要翻译: 本发明涉及一种催化剂,特别是用于通过邻二甲苯和/或萘的气相氧化制备邻苯二甲酸酐,其具有惰性载体和至少一层已被施加到其上并具有催化活性组合物,该组合物包含 TiO 2,其特征在于所用的TiO 2的至少一部分具有以下性质:(a)BET表面积大于15m 2 / g,(b)总孔体积的至少25%由具有 半径在60和400nm之间,(c)主晶体尺寸大于22μm。 还描述了制备这种催化剂的优选方法,以及根据本发明使用的二氧化钛的优选用途。
-
-
-