Continuous casting mold for billet
    1.
    发明授权
    Continuous casting mold for billet 失效
    坯料连铸模具

    公开(公告)号:US6112805A

    公开(公告)日:2000-09-05

    申请号:US473085

    申请日:1999-12-28

    摘要: Recess portions each comprising one or a plurality of transverse grooves or a large number of dimples are disposed below the lowermost position of a meniscus under a steady operation state within a distance of 200 mm on the inner peripheral surface of the casting mold so that a solidified shell is gradually cooled and the cooling capacity of each inner surface of the casting mold is substantially inform.

    摘要翻译: 在铸模的内周面上的距离为200mm的稳定运行状态下,在弯液面的最下位置的下方配置有包含一个或多个横槽或多个凹部的凹部, 壳体逐渐冷却,并且浇铸模具的每个内表面的冷却能力基本上被通知。

    Continuous casting method for billet
    2.
    发明授权
    Continuous casting method for billet 失效
    坯料连铸方法

    公开(公告)号:US6024162A

    公开(公告)日:2000-02-15

    申请号:US702611

    申请日:1996-11-21

    摘要: To provide a continuous casting method for a billet capable of stable casting without causing rhomboidity or side periphery deformation in the billet produced by continuous casting, in a casting mold used for this method, recess portions each comprising one or a plurality of transverse grooves or a large number of dimples are disposed below the lowermost position of a meniscus under a steady operation state within a distance of 200 mm on the inner peripheral surface of the casting mold so that a solidified shell is gradually cooled and the cooling capacity of each inner surface of the casting mold is substantially uniform.